Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50到0.70 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.15 | % |
Moisture Absorption | Equilibrium,23°C | ASTMD570 | 0.35 | % |
Moisture Absorption | Equilibrium,100°C | ASTMD570 | 0.58 | % |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 11 | g/10min |
Specific Volume | | ASTMD792 | 0.830 | cm³/g |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17Wheel | ASTMD1044 | 10.0 | mg |
Tensile Elongation | Yield | ASTMD638 | 7.0 | % |
Tensile Elongation | Break | ASTMD638 | 130 | % |
Tensile Strength | Yield | ASTMD638 | 62.0 | Mpa |
Tensile Strength | Break | ASTMD638 | 68.0 | Mpa |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 2340 | Mpa |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 96.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Vicat Softening Temperature | | ASTMD15256 | 154 | °C |
Specific Heat | | ASTMC351 | 1250 | J/kg/°C |
Thermal Conductivity | | ASTMC177 | 0.27 | W/m/K |
Linear thermal expansion coefficient | MD:-40to95°C | ASTME831 | 6.8E-05 | cm/cm/°C |
Deflection Temperature Under Load? | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 137 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed,6.40mm | ASTMD648 | 132 | °C |
RTIElec | | UL746 | 130 | °C |
Evolution Calendar intelligent importer | | UL746 | 130 | °C |
RTI | | UL746 | 130 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dissipation Factor? | 50Hz | ASTMD150 | 9E-04 | |
Dissipation Factor? | 60Hz | ASTMD150 | 9E-04 | |
Dissipation Factor? | 1MHz | ASTMD150 | 0.010 | |
Dielectric Constant | 1MHz | ASTMD150 | 2.96 | |
Dielectric Constant | 50Hz | ASTMD150 | 3.17 | |
Dielectric Constant | 60Hz | ASTMD150 | 3.17 | |
Volume Resistivity | | ASTMD257 | >1.0E+17 | ohms·cm |
Dielectric Strength | 3.20mm,inAir | ASTMD149 | 15 | KV/mm |
Comparative Tracking Index | CTI | UL746 | PLC2 | |
Hot-wire Ignition | HWI | UL746 | PLC2 | |
High Amp Arc Ignition | HAI | UL746 | PLC1 | |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC2 | |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Gardner Impact | 23°C | ASTMD3029 | 169 | J |
Unnotched Izod Impact Strength | 23°C | ASTMD4812 | 3200 | J/m |
Tensile Impact Strength | | ASTMD1822 | 577 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | M-Scale | ASTMD785 | 70 | |
Rockwell Hardness | R-Scale | ASTMD785 | 118 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Transmittance | 2540µm | ASTMD1003 | 88.0 | % |
Haze | 2540µm | ASTMD1003 | 1.0 | % |
Refractive index of light | | ASTMD542 | 1.586 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Glow Wire Ignition Temperature | 1.0mm | IEC60695-2-13 | 875 | °C |
Oxygen Index | | ASTMD2863 | 25 | % |
UL flame retardant rating | 1.5mm | UL94 | V-2 | |
Glow Wire Flammability Index | 1.0mm | IEC60695-2-12 | 850 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.