Need Help? Contact Us service@plas.com
Get App

PC LEXAN™  4019 SABIC INNOVATIVE US

71
  • Unit Price:
    $3111 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    20MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Middle flow Thermal stability
  • Application Areas:Electronic display Lighting applications
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageMD:3.20mm内部方法0.20to0.60%
Modeling ShrinkageTD:3.20mm内部方法0.20to0.60%
Moisture AbsorptionSaturation,23°CISO620.15%
Moisture AbsorptionEquilibrium,23°C,50%RHISO620.40%
Melt Mass-Flow Rate300°C/1.2kgASTMD12387.5g/10min
Melt Volume flow Rate300°C/1.2kgISO11336.50cm3/10min
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Flexural StrengthISO17898.0Mpa
Tensile ModulusISO527-2/13900Mpa
Tensile ElongationBreakASTMD63814%
Flexural ModulusISO1783450Mpa
Tensile StressYieldISO527-2/554.0Mpa
Tensile StressBreakISO527-2/548.0Mpa
Tensile StrainYieldISO527-2/54.3%
Tensile StrainBreakISO527-2/58.7%
Tensile ElongationYieldASTMD6384.3%
Tensile ModulusASTMD6383950Mpa
Tensile StrengthBreakASTMD63845.0Mpa
Tensile StrengthYieldASTMD63855.0Mpa
Flexural Modulus50.0mmSpanASTMD7903500Mpa
Flexural StrengthYield,50.0mmSpanASTMD790103Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Linear thermal expansion coefficientMD:-40to40°CISO11359-24.7E-05cm/cm/°C
Linear thermal expansion coefficientTD:-40to40°CASTME8317E-05cm/cm/°C
Linear thermal expansion coefficientTD:-40to40°CISO11359-27E-05cm/cm/°C
Linear thermal expansion coefficientMD:-40to40°CASTME8314.7E-05cm/cm/°C
Deflection Temperature Under Load?1.8MPa,Unannealed,3.20mmASTMD648137°C
Vicat Softening TemperatureASTMD152510146°C
Vicat Softening Temperature--ISO306/B50146°C
Vicat Softening Temperature--ISO306/B120146°C
Ball PressureTest75°CIEC60695-10-2Pass
Heat Deflection Temperature1.8MPa,Unannealed,100mmSpanISO75-2/Ae135°C
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Charpy Notched Impact Strength-30°CISO179/1eA15kJ/m²
Charpy Notched Impact Strength23°CISO179/1eA25kJ/m²
Charpy Unnotched Impact Strength-30°CISO179/1eUNoBreak
Charpy Unnotched Impact Strength23°CISO179/1eUNoBreak
Notched Izod Impact Strength-30°CISO180/1A10kJ/m²
Notched Izod Impact Strength23°CISO180/1A25kJ/m²
Unnotched Izod Impact Strength-30°CISO180/1UNoBreak
Unnotched Izod Impact Strength23°CISO180/1UNoBreak
Instrumented Dart Impact23°C,TotalEnergyASTMD376340.0J
FlammabilityTest ConditionTest MethodTest ResultUnit
Flame Rating0.75mmUL94HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.