PA66 Ultramid® A3EG6 BASF USA
108
- Unit Price:
- $4543 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High rigidity Oil resistant dimensional stability
- Application Areas:Electrical components Electronic insulation machine Mechanical components Shell
- Color:--
- Grade:Enhanced level
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | Saturation, 23°C | ISO 62 | 5.2 到 5.8 | % |
Equilibrium, 23°C, 50% RH | ISO 62 | 1.5 到 1.9 | % | |
Apparent Density | 0.70 | g/cm³ | ||
Viscosity number | 96% H2SO4 | ISO 307 | 145 | cm³/g |
Melt Volume flow Rate | 275°C/5.0 kg | ISO 1133 | 40.0 | cm3/10min |
Modeling Shrinkage | 0.55 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Creep Modulus | 1000 hr | ISO 899-1 | -- | Mpa |
Flexural Stress | ISO 178 | 280 | Mpa | |
Tensile Stress | Break | ISO 527-2 | 190 | Mpa |
Tensile Strain | Break | ISO 527-2 | 3.0 | % |
Tensile Modulus | ISO 527-2 | 10000 | Mpa | |
Flexural Modulus | ISO 178 | 8600 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45 MPa, Unannealed | ISO 75-2/B | 250 | °C |
1.8 MPa, Unannealed | ISO 75-2/A | 250 | °C | |
Specific Heat | 1500 | J/kg/°C | ||
Thermal Conductivity | DIN 52612 | 0.35 | W/m/K | |
Temperature Index | -- 5 | IEC 60216 | 165 | °C |
-- 6 | IEC 60216 | 135 | °C | |
Melting temperature | ISO 11357-3 | 260 | °C | |
Maximum Service Temperature (short cycle operation) | 240 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Relative Permittivity | 1 MHz | IEC 60250 | 3.50 | |
Comparative Tracking Index | Solution A | IEC 60112 | 550 | V |
Dissipation Factor? | 1 MHz | IEC 60250 | 0.014 | |
Surface Resistivity | IEC 60093 | -- | ohms | |
Volume Resistivity | IEC 60093 | 1.0E+15 | ohms·cm |
Injection | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Processing (Melt) Temp | 280 到 300 | °C | ||
Mold Temperature | 80 到 90 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO 179/1eU | 70 | kJ/m² |
23°C | ISO 179/1eU | 85 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flammability level | 1.6 mm | IEC 60695-11-10, -20 | HB | |
Polymer Abbreviation | PA66-GF30 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.