PA6 LNP™ LUBRICOMP™ PX11311 WH9F059 SABIC INNOVATIVE US
145
- Unit Price:
- $6058 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Dimensional stability Low Specific Gravity
- Application Areas:Automotive body panels Automotive sector
- Color:--
- Grade:Impact resistant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:24hr | ASTMD955 | 0.33 | % |
TD:24hr | ASTMD955 | 0.48 | % | |
Melt Volume flow Rate | 300°C/10.0kg | ISO1133 | 49.0 | cm3/10min |
23°C,24hr | 内部方法 | 0.25 | % | |
Equilibrium,23°C,50%RH | ISO62 | 0.040 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Modulus | ASTMD638 | 7240 | Mpa | |
Flexural Strength | Break,50.0mmSpan | ASTMD790 | 76.0 | Mpa |
Tensile Strength | Break | ASTMD638 | 52.0 | Mpa |
Tensile Elongation | Break | ASTMD638 | 2.0 | % |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 9050 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed,6.40mm | ASTMD648 | 199 | °C |
Linear thermal expansion coefficient | MD:-40to40°C | ASTME831 | 3.1E-05 | cm/cm/°C |
MD:40to120°C | ASTME831 | 1.9E-05 | cm/cm/°C | |
TD:-40to40°C | ASTME831 | 4.6E-05 | cm/cm/°C | |
TD:40to120°C | ASTME831 | 7E-05 | cm/cm/°C | |
Specific Heat | ASTMC351 | 1420 | J/kg/°C | |
--6 | ASTM D790/ISO 178 | 1.2 | W/m/K | |
--7 | ASTM D790/ISO 178 | 2.1 | W/m/K | |
--8 | ISO22007-2 | 0.99 | W/m/K | |
--9 | ISO22007-2 | 1.4 | W/m/K |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation Factor? | 1.10GHz | ASTMES7-83 | 7.7E-03 | |
Dielectric Strength | 1.00mm,inOil | ASTMD149 | >10 | KV/mm |
Comparative Tracking Index | IEC60112 | 600 | V | |
Surface Resistivity | ASTMD257 | >1.0E+15 | ohms | |
Dielectric Constant | 1.10GHz | ASTMES7-83 | 4.74 | |
Hot-wire Ignition | HWI | UL746 | PLC0 | |
High Amp Arc Ignition | HAI | UL746 | PLC0 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | ISO179 | 5.3到18 | kJ/m² | |
Unnotched Izod Impact Strength | 23°C | ASTMD4812 | 180 | J/m |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Glow Wire Ignition Temperature | 1.00mm | IEC60695-2-13 | 775 | °C |
3.00mm | IEC60695-2-13 | 850 | °C | |
UL flame retardant rating | 1.00mm | UL94 | V-0 | |
Glow Wire Flammability Index | 2.00mm | IEC60695-2-12 | 960 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.