PA6 Ultramid® B3EG3 BASF GERMANY
246
- Unit Price:
- $3589 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 69MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Oil resistant High impact resistance Filler: Glass fiber reinf 15% filler by weight
- Application Areas:wheel Automotive sector Shell wheel Application in the automo Shell
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density/specific gravity | ISO1183 | 1.23 | g/cm³ | |
Water absorption rate | Saturation,23°C | ISO62 | 7.7 | % |
Equilibrium,23°C,50%RH | ISO62 | 2.3 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | 23°C | ISO527-2 | 6060 | Mpa |
Bending modulus | 23°C | ISO178 | 5300 | Mpa |
Tensile stress | Break,23°C | ISO527-2 | 115 | Mpa |
Tensile strain | Break,23°C | ISO527-2 | 2.5 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO75-2/B | 217 | °C |
1.8MPa,Unannealed | ISO75-2/A | 200 | °C | |
Melting temperature (DSC) | ISO3146 | 220 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric constant | 1MHz | IEC60250 | 3.80 | |
Volume resistivity | IEC60093 | 1E+13 | ohms·cm | |
Dissipation factor | 100Hz | IEC60250 | 0.025 | |
1MHz | IEC60250 | 0.025 |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO179 | 5.0 | kJ/m² |
Impact strength of cantilever beam gap | -30°C | ISO180 | 4.5 | kJ/m² |
23°C | ISO180 | 5.0 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.