Technical Data Sheet
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod Impact Strength | 23℃ | ISO 180/A | 2 | kJ/m² |
物理性能 | Test Condition | Test Method | Test Result | Unit |
---|
Melt Volume flow Rate | | ISO 1133 | 23 | cm3/10min |
Density | | ISO 1183 | 1.08 | g/cm³ |
Modeling Shrinkage | | ISO 294-4 | 0.3-0.4 | % |
机械性能 | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | Yield,23℃ | ISO 527 | 68 | Mpa |
Flexural Strength | | ISO 178 | 111 | Mpa |
Flexural Modulus | | ISO 178 | 3800 | Mpa |
Tensile Modulus | | ISO 527 | 3700 | Mpa |
Tensile Strain | Break,23℃ | ISO 527 | 3.2 | % |
Rockwell Hardness | R-Scale | ISO 2039-2 | 126 | |
Optical | Test Condition | Test Method | Test Result | Unit |
---|
Transmittance | | ASTM D1003 | 87-88 | % |
Thermal | Test Condition | Test Method | Test Result | Unit |
---|
Vicat Softening Temperature | B120 | ASTM D1525 | 104 | °C |
Heat Deflection Temperature | Annealed,1.80 MPa | ISO 75 | 101 | °C |
Heat Deflection Temperature | Annealed,0.45MPa | ISO 75 | 103 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.