Need Help? Contact Us service@plas.com
Get App

ABS ECO GP-22 MR70 INEOS STYRO KOREA

137
  • Unit Price:
    $2109 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Impact resistance Heat resistant deformatio
  • Application Areas:Electrical enclosure electronic product Household appliances
  • Color:--
  • Grade:--

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageISO294-40.40to0.70%
Modeling ShrinkageMDASTMD9550.40to0.70%
Moisture AbsorptionEquilibrium,23°C,50%RHISO620.22%
Moisture AbsorptionSaturation,23°CISO621.0%
Moisture AbsorptionSaturation,23°CASTMD5701.0%
Melt Mass-Flow Rate220°C/10.0kgASTMD123819g/10min
Melt Mass-Flow Rate200°C/5.0kgASTMD12381.5g/10min
Melt Volume flow Rate220°C/10.0kgISO113319.0cm3/10min
Melt Volume flow Rate230°C/3.8kgASTMD12384.80cm3/10min
Density / Specific GravityISO11831.04g/cm³
Density / Specific GravityASTMD7921.04g/cm³
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Nominal Tensile Strain at Break23°CISO527-210%
Flexural StressISO17865.0Mpa
Tensile StrengthYield,23°CASTMD63845.0Mpa
Tensile StressYield,23°CISO527-245.0Mpa
Tensile StrainYield,23°CISO527-22.6%
Tensile ModulusISO527-22300Mpa
Tensile ModulusASTMD6382300Mpa
Tensile ElongationBreakASTMD6382.6%
Flexural ModulusASTMD7902300Mpa
Flexural StrengthASTMD79065.0Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Deflection Temperature Under Load?1.8MPa,UnannealedASTMD64877.8°C
Deflection Temperature Under Load?1.8MPa,AnnealedASTMD64898.9°C
Deflection Temperature Under Load?0.45MPa,UnannealedASTMD64890.6°C
Deflection Temperature Under Load?0.45MPa,AnnealedASTMD648104°C
Vicat Softening Temperature--ISO306/A50105°C
Vicat Softening Temperature--ISO306/B5096.0°C
Linear thermal expansion coefficientMDISO11359-28.0E-5to1.1E-4cm/cm/°C
Heat Deflection Temperature1.8MPa,AnnealedISO75-2/A94.0°C
Heat Deflection Temperature0.45MPa,AnnealedISO75-2/B99.0°C
Thermal ConductivityDIN526120.17W/m/K
Electrical performanceTest ConditionTest MethodTest ResultUnit
Dissipation Factor?100HzIEC602504.8E-03
Dissipation Factor?1MHzIEC602507.9E-03
Relative Permittivity100HzIEC602502.90
Relative Permittivity1MHzIEC602502.80
Surface ResistivityIEC600931E+13ohms
Dielectric Constant1.00mm,1MHzASTMD1502.80
Volume ResistivityASTMD257>1.0E+15ohms·cm
Volume ResistivityIEC600931E+15ohms·cm
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Charpy Unnotched Impact Strength-30°CISO179100kJ/m²
Charpy Unnotched Impact Strength23°CISO179180kJ/m²
Charpy Notched Impact Strength23°CISO17922kJ/m²
Charpy Notched Impact Strength-30°CISO1798.0kJ/m²
Notched Izod Impact Strength-30°CASTMD25659J/m
Notched Izod Impact Strength-18°CASTMD256100J/m
Notched Izod Impact Strength23°CASTMD256300J/m
Notched Izod Impact Strength-30°CISO180/A8.0kJ/m²
Notched Izod Impact Strength23°CISO180/A26kJ/m²
hardnessTest ConditionTest MethodTest ResultUnit
Rockwell HardnessR-ScaleASTMD785103
Ball Indentation HardnessISO2039-197.0Mpa
optical performance Test ConditionTest MethodTest ResultUnit
The Yellow IndexDIN616713YI
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.