ABS Novodur® H801 901510 INEOS STYRO THAILAND
140
- Unit Price:
- $3374 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:Application in the automo Automotive interior parts Automotive interior equip
- Color:--
- Grade:Heat resistant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density / Specific Gravity | ISO1183 | 1.07 | g/cm³ | |
Melt Mass-Flow Rate | 220℃/10.0Kg | ISO1133 | 9 | g/10min |
线性收缩率 | ISO294-4 | 0.5-0.7 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Modulus | 23°C | ISO178 | 2300 | Mpa |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 60 | kJ/m² |
-30°C | ISO179/1eA | 12 | kJ/m² | |
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 220 | kJ/m² |
-30°C | ISO179/1eU | 160 | kJ/m² | |
Notched Izod Impact Strength | 23°C | ISO180/1A | 30 | kJ/m² |
-30°C | ISO180/1A | 12 | kJ/m² | |
Tensile Strength | Yield,23°C | ISO527-2 | 49 | Mpa |
Tensile Elongation?(Break) | Yield,23°C | ISO527-2 | 3 | % |
23°C | ISO527-2 | >=15 | % | |
Tensile Modulus | 23°C | ISO527-2 | 2400 | Mpa |
Flexural Strength | 23°C | ISO178 | 77 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Coefficient of Linear Thermal Expansion | MD | ISO11359-2 | 8E-05 | cm/cm/°C |
Deflection Temperature Under Load? | 0.45MPaUnannealed | ISO75-2/Bf | 106 | °C |
1.80MPaAnnealed | ISO75-2/Af | 99 | °C | |
Vicat Softening Temperature | 5.10kg | ISO306/A50 | 105 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Volume Resistivity | IEC60093 | 1E+14 | Ω.cm | |
Surface resistance | IEC60093 | 1E+16 | Ω.cm | |
Insulation strength | 1.00mm | IEC60243-1 | 38 | KV/mm |
Dielectric Constant | IEC60250 | 3 | 1MHz | |
IEC60250 | 3.1 | 100HZ | ||
Dissipation Factor? | IEC60250 | 0.05 | ||
IEC60250 | 0.09 | |||
相对漏电起痕指数 | IEC60112 | 600 | V |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Ball Indentation Hardness | ISO2039-1 | 105 | Mpa |
Flame Rating | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Glow Wire Ignition Temperature | 2.00mm | IEC60695-2-12 | 700 | °C |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melting temperature | ISO294 | 240 | °C | |
Injection Rate | ISO294 | 240 | mm/sec | |
Burning rate | ISO3795 | 45 | mm/min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.