ABS Toyolac® 100-322 TORAY MALAYSIA
72
- Unit Price:
- $2164 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 31MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Glass fiber reinforced High impact resistance
- Application Areas:Electronic and electrical household electrical appl
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 0.40到0.60 | % |
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.30 | % |
Melt Mass-Flow Rate | 220°C/10.0kg | ISO1133 | 15 | g/10min |
Density / Specific Gravity | ASTMD792,ISO1183 | 1.04 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Yield | ASTMD638 | 48.0 | Mpa | |
--4 | ASTMD790 | 74.0 | Mpa | |
Flexural Modulus | ASTMD790 | 2280 | Mpa | |
Tensile Modulus | ISO527-2/1 | 2600 | Mpa | |
yield | ISO527-2/50 | 51.0 | Mpa | |
fracture | ISO527-2/50 | >10 | % | |
--5 | ISO178 | 78.0 | Mpa | |
Break | ASTMD638 | 48 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
1.8MPa, Unannealed,6.40mm | ASTMD648 | 88.0 | °C | |
1.8MPa,未退火,12.7mm | ASTMD648 | 93.0 | °C | |
Thermal Conductivity | ASTMC177 | 0.15 | W/m/K | |
1.8MPa, Unannealed | ISO75-2/A | 83.0 | °C | |
Linear thermal expansion coefficient | MD | ASTMD696 | 7.4E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Strength | ASTMD149 | 23 | KV/mm | |
Surface Resistivity | ASTMD257 | >1.0E+16 | ohms | |
Dielectric Constant | 1kHz | ASTMD150 | 3.10 | |
Volume Resistivity | 23°C | ASTMD257 | >1.0E+16 | ohms·cm |
Dissipation Factor? | 1kHz | ASTMD150 | 6.6E-03 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 20 | kJ/m² |
Notched Izod Impact Strength | -30°C,3.20mm | ASTMD256 | 140 | J/m |
-30°C,12.7mm | ASTMD256 | 120 | J/m | |
0°C,3.20mm | ASTMD256 | 200 | J/m | |
0°C,12.7mm | ASTMD256 | 180 | J/m | |
23°C,3.20mm | ASTMD256 | 270 | J/m | |
23°C,12.7mm | ASTMD256 | 230 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 112 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.