Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:--1 | 内部方法 | 0.50到0.70 | % |
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50到0.70 | % |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 22 | g/10min |
Melt Volume flow Rate | 300°C/1.2kg | ISO1133 | 21.0 | cm3/10min |
Saturation ,23℃ | | ISO62 | 0.35 | % |
Saturation ,23℃ | | ASTMD570 | 0.35 | % |
Density / Specific Gravity | | ASTMD792,ISO1183 | 1.20 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
-- | | ISO527-2/1 | 2350 | Mpa |
--2 | | ASTMD638 | 2350 | Mpa |
Yield | | ASTMD638 | 63.0 | Mpa |
50.0mm Span | | ASTMD790 | 2300 | Mpa |
--7 | | ISO178 | 2300 | Mpa |
--8 | | ISO178 | 90.0 | Mpa |
Yield | | ASTMD638 | 6.0 | % |
Break | | ASTMD638 | >70 | % |
Yield,50.0mm Span | | ASTMD790 | 90.0 | Mpa |
yield | | ISO527-2/50 | 6.0 | % |
yield | | ISO527-2/50 | 63.0 | Mpa |
fracture | | ISO527-2/50 | >70 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Ball PressureTest | 125°C | IEC60695-10-2 | Pass | |
Thermal Conductivity | | ASTMC177,ISO8302 | 0.20 | W/m/K |
Vicat Softening Temperature | | ISO306/B50,ASTMD152515 | 140 | °C |
1.8MPa, Unannealed,3.20mm | | ASTMD648 | 122 | °C |
0.45MPa, Unannealed,3.20mm | | ASTMD648 | 133 | °C |
-40到95°C | | ASTME831 | 7E-05 | cm/cm/°C |
23到80°C | | ISO11359-2 | 7E-05 | cm/cm/°C |
1.8MPa, Unannealed,64.0mm Span | | ISO75-2/Af | 122 | °C |
0.45MPa, Unannealed,3.20mm Span | | ISO75-2/Bf | 133 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dissipation Factor? | 60Hz | ASTMD150,IEC60250 | 1E-03 | |
Dissipation Factor? | 1MHz | ASTMD150,IEC60250 | 0.010 | |
Dielectric Strength | 1.60mm | ASTMD149,IEC60243-1 | 27 | KV/mm |
Dielectric Constant | 60Hz | ASTMD150,IEC60250 | 3.00 | |
Dielectric Constant | 1MHz | ASTMD150,IEC60250 | 3.00 | |
Volume Resistivity | | ASTMD257,IEC60093 | >1.0E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 55.0 | J |
-30°C12 | | ISO180/1U | 无断裂 | |
-30°C10 | | ISO180/1A | 12 | kJ/m² |
23°C11 | | ISO180/1A | 65 | kJ/m² |
23°C | | ASTMD256 | 640 | J/m |
23°C | | ASTMD4812,ISO180/1U | 无断裂 | |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness (R-Scale) | | ASTMD785 | 120 | |
R-Scale | | ISO2039-2 | 120 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Refractive index of light | | ASTMD542,ISO489 | 1.586 | |
Haze | 2540µm | ASTMD1003 | <0.80 | % |
Transmittance | 2540µm | ASTMD1003 | 88.0到90.0 | % |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 1.60mm | UL94 | V-2 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.