ASIA PLASTIC EXCHANGE LIMITED
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 0.60 | % |
TD | ASTMD955 | 0.60 | % | |
Moisture Absorption | 24hr | ASTMD570 | 0.20 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Break,23°C | ISO527-2 | 160 | Mpa |
Break,24°C | ISO527-2 | 65.5 | Mpa | |
Tensile Strain | Break,23°C | ISO527-2 | 3.7 | % |
Break,24°C | ISO527-2 | 4.2 | % | |
Tensile Modulus | ASTMD638 | 6480 | Mpa | |
23°C | ISO527-2 | 6890 | Mpa | |
100°C | ISO527-2 | 6690 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 3.8 | % |
Flexural Modulus | ASTMD790 | 6000 | Mpa | |
23°C | ISO178 | 6690 | Mpa | |
100°C | ISO178 | 4960 | Mpa | |
Flexural Strength | ASTMD790 | 226 | Mpa | |
Flexural Stress | 23°C | ISO178 | 197 | Mpa |
100°C | ISO178 | 141 | Mpa | |
Compressive Strength | ASTMD695 | 124 | Mpa | |
Shearing Strength | ASTMD732 | 69.6 | Mpa | |
Tensile Strength | ASTMD638 | 161 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Peak Melting Temperature | ASTMD3418 | 310 | °C | |
Linear thermal expansion coefficient | MD:0to100°C | ASTME831 | 2.2E-05 | cm/cm/°C |
MD:100to200°C | ASTME831 | 1.6E-05 | cm/cm/°C | |
TD:0to100°C | ASTME831 | 7.5E-05 | cm/cm/°C | |
TD:100to200°C | ASTME831 | 1.2E-04 | cm/cm/°C | |
Deflection Temperature Under Load? | 0.45MPa,Annealed | ASTMD648 | 268 | °C |
1.8MPa,Unannealed | ISO75-2/A | 258 | °C | |
1.8MPa,Annealed | ASTMD648 | 254 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 86 | kJ/m² |
Notched Izod impact strength | 23°C | ISO180/1U | 53 | kJ/m² |
Instrumented Dart Impact | EnergyatMaxumumLoad2 | ASTMD3763 | 1.76 | J |
EnergyatMaxumumLoad3 | ASTMD3763 | -- | J | |
TotalEnergy | ASTMD3763 | 10.0 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.