Material Description
Technical Data Sheet
Material Description
- Material Properties:heat-resisting optical performance High impact resistance
- Application Areas:sheet sheet
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 0.50to0.70 | % |
MD | ISO294-4 | 0.50to0.70 | % | |
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.15 | % |
23°C,24hr | ISO62 | 0.15 | % | |
Equilibrium,23°C,50%RH | ASTMD570 | 0.32 | % | |
Equilibrium,23°C,50%RH | ISO62 | 0.32 | % | |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 5.0 | g/10min |
300°C/1.2kg | ISO1133 | 5.0 | g/10min | |
Density / Specific Gravity | ASTMD792 | 1.20 | g/cm³ | |
ISO1183/B | 1.20 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Modulus | ISO527-2/50 | 2400 | Mpa | |
Flexural Modulus | ASTMD790 | 2340 | Mpa | |
Tensile Strength | Yield | ASTMD638 | 60.7 | Mpa |
Break | ASTMD638 | 71.7 | Mpa | |
Tensile Elongation | Yield | ASTMD638 | 6.0 | % |
Break | ASTMD638 | 170 | % | |
Flexural Strength | ASTMD790 | 93.8 | Mpa | |
Flexural Stress | ISO178 | 94.0 | Mpa | |
Tensile Modulus | ASTMD638 | 2410 | Mpa | |
Flexural Modulus | ISO178 | 2350 | Mpa | |
Tensile Stress | Yield | ISO527-2/50 | 61.0 | Mpa |
Break | ISO527-2/50 | 72.0 | Mpa | |
Tensile Strain | Yield | ISO527-2/50 | 6.0 | % |
Break | ISO527-2/50 | 170 | % | |
TaberAbrasionResistance5 | ASTMD1044 | 5 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear thermal expansion coefficient | MD:-40to82°C | ASTMD696 | 6.8E-05 | cm/cm/°C |
Glass Transition Temperature | ISO11357-2 | 150 | °C | |
ASTMD3418 | 150 | °C | ||
Vicat Softening Temperature | -- | ASTMD15256 | 148 | °C |
-- | ASTMD15257 | 154 | °C | |
-- | ISO306/A120 | 154 | °C | |
-- | ISO306/B50 | 148 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 71 | kJ/m² |
23°C | ISO179/1eA | 81 | kJ/m² | |
Notched Izod Impact Strength | -30°C | ASTMD256 | 590 | J/m |
23°C | ASTMD256 | 910 | J/m |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Haze | ASTMD1003 | 1.0 | % | |
Transmittance | ASTMD1003 | 86.0to90.0 | % | |
Refractive index of light | ASTMD542 | 1.586 | ||
ISO489 | 1.586 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flame Rating | 1.5mm | UL94 | HB | |
3.0mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.