ABS/PC CYCOLOY™ XCY630L-BK1566U SABIC INNOVATIVE US
90
- Unit Price:
- $4571 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50to0.70 | % |
TD:3.20mm | 内部方法 | 0.50to0.70 | % | |
Moisture Absorption | Saturation,23°C | ISO62 | 0.40 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.15 | % | |
Melt Mass-Flow Rate | 260°C/5.0kg | ASTMD1238 | 26 | g/10min |
Melt Volume flow Rate | 260°C/5.0kg | ISO1133 | 22.0 | cm3/10min |
Melt Viscosity | 260°C,1500sec^-1 | ISO11443 | 170 | Pa·s |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Elongation | Yield | ASTMD638 | 4.5 | % |
Tensile Modulus | ASTMD638 | 2300 | Mpa | |
Tensile Strength | Yield | ASTMD638 | 54.0 | Mpa |
Break | ASTMD638 | 53.0 | Mpa | |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 2300 | Mpa |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 89.0 | Mpa |
Tensile Elongation | Break | ASTMD638 | 120 | % |
Flexural Modulus | ISO178 | 2200 | Mpa | |
Flexural Strength | ISO178 | 82.0 | Mpa | |
Tensile Modulus | ISO527-2/1 | 2250 | Mpa | |
Tensile Stress | Break | ISO527-2/50 | 53.0 | Mpa |
Yield | ISO527-2/50 | 54.0 | Mpa | |
Tensile Strain | Yield | ISO527-2/50 | 4.5 | % |
Break | ISO527-2/50 | 120 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear thermal expansion coefficient | MD:-40to40°C | ASTME831 | 7E-05 | cm/cm/°C |
MD:-40to40°C | ISO11359-2 | 8E-05 | cm/cm/°C | |
TD:-40to40°C | ASTME831 | 7E-05 | cm/cm/°C | |
TD:-40to40°C | ISO11359-2 | 8E-05 | cm/cm/°C | |
Deflection Temperature Under Load? | 1.8MPa,Unannealed,3.20mm | ASTMD648 | 107 | °C |
Thermal Conductivity | ISO8302 | 0.20 | W/m/K | |
Ball PressureTest | 75°C | IEC60695-10-2 | Pass | |
Heat Deflection Temperature | 0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 126 | °C |
1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 105 | °C | |
Vicat Softening Temperature | ASTMD152510 | 126 | °C | |
-- | ISO306/B50 | 126 | °C | |
-- | ISO306/B120 | 127 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface Resistivity | IEC60093 | >1.0E+15 | ohms | |
Volume Resistivity | IEC60093 | >1.0E+15 | ohms·cm | |
Dielectric Strength | 0.800mm,in Oil | IEC60243-1 | 35 | KV/mm |
1.60mm,in Oil | IEC60243-1 | 25 | KV/mm | |
3.20mm,in Oil | IEC60243-1 | 17 | KV/mm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 30 | kJ/m² |
23°C | ISO179/1eA | 65 | kJ/m² | |
Notched Izod Impact Strength | -30°C | ISO180/1A | 30 | kJ/m² |
23°C | ISO180/1A | 65 | kJ/m² | |
Instrumented Dart Impact | -30°C,TotalEnergy | ASTMD3763 | 67.0 | J |
23°C,TotalEnergy | ASTMD3763 | 55.0 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.