PPSU RADEL® R-5100 BU525 SOLVAY JAPAN
161
- Unit Price:
- $27746 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 20MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Resistance to stress crac Thermal stability High impact resistance
- Application Areas:Electrical applications household electrical appl Medical devices
- Color:--
- Grade:--
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 0.70 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.37 | % |
Melt Mass-Flow Rate | ASTMD1238 | 14to20 | g/10min | |
Density / Specific Gravity | ASTMD792 | 1.30 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Compressive Modulus | ASTMD695 | 1730 | Mpa | |
Compressive Strength | ASTMD695 | 98.9 | Mpa | |
Shearing Strength | ASTMD732 | 62.7 | Mpa | |
Poisson Ratio | ASTME132 | 0.42 | ||
Tensile Strength | Yield | ASTMD638 | 69.6 | Mpa |
Break | ASTMD638 | 69.6 | Mpa | |
Tensile Modulus | ASTMD638 | 2340 | Mpa | |
Tensile Elongation | Yield | ASTMD638 | 7.2 | % |
Break | ASTMD638 | 60 | % | |
Flexural Modulus | ASTMD790 | 2410 | Mpa | |
Flexural Strength | Yield | ASTMD790 | 91.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ASTMD648 | 214 | °C |
1.8MPa,Unannealed | ASTMD648 | 207 | °C | |
Glass Transition Temperature | ASTME1356 | 220 | °C | |
Thermal Conductivity | ASTMC177 | 0.35 | W/m/K | |
Linear thermal expansion coefficient | MD | ASTMD696 | 5.6E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Strength | ASTMD149 | 14 | KV/mm | |
Dielectric Constant | 60Hz | ASTMD150 | 3.44 | |
1kHz | ASTMD150 | 3.40 | ||
Volume Resistivity | ASTMD257 | 9E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Impact Strength | ASTMD1822 | 399 | kJ/m² | |
Notched Izod Impact Strength | ASTMD256 | 690 | J/m | |
ASTMD256 | NoBreak |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Refractive index of light | ASTMD542 | 1.672 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Oxygen Index | ASTMD2863 | 38 | % | |
Flame Rating | 0.75mm,ALLcolors,ULfileE36098 | UL94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.