ABS/PMMA STAREX® BF-0670 BK22101 Samsung Cheil South Korea
171
- Unit Price:
- $2227 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 51MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High temperature resistan Aging resistance High impact resistance
- Application Areas:Electrical appliances Electronic and electrical Automotive components Lighting fixtures
- Color:--
- Grade:--
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Mass-Flow Rate | 220°C/10.0kg | ASTMD1238 | 25 | g/10min |
220°C/10.0kg | ISO1133 | 24 | g/10min | |
Modeling Shrinkage | MD:3.20mm | ASTMD955 | 0.30 | % |
TD:3.20mm | ASTMD955 | 0.30 | % | |
TD:3.20mm | ISO2577 | 0.40 | % | |
MD:3.20mm | ISO2577 | 0.40 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Yield | ISO527-2/50 | 52.0 | Mpa |
Break | ISO527-2/50 | 36.0 | Mpa | |
Tensile Strain | Break | ISO527-2/50 | 22 | % |
Tensile Modulus | ASTMD638 | 2080 | Mpa | |
Flexural Modulus | ISO178 | 2360 | Mpa | |
Flexural Modulus | ASTMD790 | 2350 | Mpa | |
Tensile Strength | Break | ASTMD638 | 36.3 | Mpa |
Yield | ASTMD638 | 49.0 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 18 | % |
Flexural Strength | ASTMD790 | 66.7 | Mpa | |
Flexural Stress | ISO178 | 70.0 | Mpa | |
Tensile Modulus | ISO527-2/50 | 2500 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed,6.40mm | ASTMD648 | 80.0 | °C |
1.8MPa,Unannealed,4.00mm | ISO75-2/A | 72.0 | °C | |
1.8MPa,Annealed,4.00mm | ISO75-2/A | 86.0 | °C | |
0.45MPa,Unannealed,6.40mm | ASTMD648 | 90.0 | °C | |
0.45MPa,Unannealed,4.00mm | ISO75-2/B | 83.0 | °C | |
0.45MPa,Annealed,4.00mm | ISO75-2/B | 92.0 | °C | |
Vicat Softening Temperature | -- | ISO306/B50 | 92.090.0 | °C |
-- | ISO306/B120 | 92.0 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod Impact Strength | 23°C | ISO180/1A | 7.4 | kJ/m² |
CharpyNotchedImpactStrength5 | 23°C | ISO179/1eA | 8.0 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 114 | |
R-Scale | ISO2039-2 | 115 | ||
Pencil Hardness | --6 | JISK5401 | F | |
--7 | JISK5401 | F |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.8mm | UL94 | HB | |
2.0mm | UL94 | HB | ||
3.0mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.