Need Help? Contact Us service@plas.com
Get App

PPO/PA NORYL GTX™  GTX910-71653 SABIC INNOVATIVE US

163
  • Unit Price:
    $4038 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:High mobility Chemical resistance High rigidity
  • Application Areas:Electrical applications electrical equipment
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageFlow : 130°C, 1hrASTM D9551.6 到 1.8%
Modeling ShrinkageFlow : 3.20 mm内部方法1.1 到 1.3%
Modeling ShrinkageAcross Flow : 3.20 mm内部方法1.0 到 1.2%
Moisture Absorption24 hr, 50% RHASTM D5700.50%
Moisture AbsorptionEquilibrium, 50% RHASTM D5701.0%
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile ElongationBreakASTM D63860%
Flexural Modulus100 mm SpanASTM D7902240Mpa
Flexural StrengthYield, 100 mm SpanASTM D79095.0Mpa
Tensile StrengthYieldASTM D63859.0Mpa
Tensile StrengthBreakASTM D63855.0Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Vicat Softening TemperatureASTM D15254232°C
Deflection Temperature Under Load?0.45 MPa, Unannealed, 6.40 mmASTM D648193°C
Deflection Temperature Under Load?1.8 MPa, Unannealed, 6.40 mmASTM D648143°C
Linear thermal expansion coefficientFlow : -40 to 95°CASTM E8319.0E-5cm/cm/°C
Linear thermal expansion coefficientFlow : 60 to 138°CASTM E8311.3E-4cm/cm/°C
Linear thermal expansion coefficientAcross Flow : -40 to 95°CASTM E8319.0E-5cm/cm/°C
Linear thermal expansion coefficientAcross Flow : 60 to 138°CASTM E8311.3E-4cm/cm/°C
RTIUL 74650.0°C
RTI ImpUL 74650.0°C
RTI ElecUL 74650.0°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
High Amp Arc IgnitionUL 746PLC 0
High Voltage Arc Tracking RateUL 746PLC 4
Arc ResistanceASTM D495PLC 7
Comparative Tracking IndexUL 746PLC 1
Hot-wire IgnitionUL 746PLC 3
InjectionTest ConditionTest MethodTest ResultUnit
Drying Time3.0 到 4.0hr
Suggested Shot Size30 到 50%
Rear Temperature265 到 305°C
Middle Temperature270 到 305°C
Front Temperature275 到 305°C
Nozzle Temperature280 到 305°C
Back Pressure0.300 到 1.40Mpa
Screw Speed20 到 100rpm
Vent Depth0.013 到 0.038mm
Drying Temperature95 到 105°C
Suggested Max Moisture0.070%
Processing (Melt) Temp280 到 305°C
Mold Temperature75 到 120°C
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Instrumented Dart Impact-30°C, Energy at PeakASTM D376339.0J
Instrumented Dart Impact23°C, Energy at PeakASTM D376350.0J
hardnessTest ConditionTest MethodTest ResultUnit
Rockwell HardnessR-ScaleASTM D785116
FlammabilityTest ConditionTest MethodTest ResultUnit
Flame Rating1.5 mmUL 94HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.