Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:3.20mm | ASTMD955 | 0.50to0.70 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.13 | % |
Moisture Absorption | 23°C,24hr | ISO62 | 0.13 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress | Yield,4.00mm | ISO527-2 | 56.0 | Mpa |
Tensile Stress | Break,4.00mm | ISO527-2 | 56.0 | Mpa |
Tensile Strain | Break,4.00mm | ISO527-2 | 130 | % |
Tensile Elongation | Yield | ASTMD638 | 6.0 | % |
Tensile Elongation | Break | ASTMD638 | 150 | % |
Flexural Modulus | | ASTMD790 | 2140 | Mpa |
Flexural Modulus | 4.00mm | ISO178 | 2100 | Mpa |
Flexural Strength | 4.00mm | ISO178 | 81.0 | Mpa |
Flexural Strength | Yield | ASTMD790 | 86.0 | Mpa |
Tensile Strength | Break | ASTMD638 | 60.0 | Mpa |
Tensile Strength | Yield | ASTMD638 | 56.0 | Mpa |
Tensile Strain | Yield,4.00mm | ISO527-2 | 5.4 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Vicat Softening Temperature | | ASTMD15252 | 118 | °C |
Vicat Softening Temperature | -- | ISO306/A | 118 | °C |
Vicat Softening Temperature | -- | ISO306/B | 110 | °C |
Specific Heat | 60°C | DSC | 1380 | J/kg/°C |
Specific Heat | 240°C | DSC | 2180 | J/kg/°C |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ASTMD648 | 103 | °C |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 103 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 90.0 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 90.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface Resistivity | | ASTMD257 | 1E+16 | ohms |
Dielectric Constant | 1kHz | ASTMD150 | 2.30 | |
Dielectric Constant | 1MHz | ASTMD150 | 2.10 | |
Arc Resistance | | ASTMD495 | 143 | sec |
Volume Resistivity | | ASTMD257 | 1E+15 | ohms·cm |
Dissipation Factor? | 1kHz | ASTMD150 | 2E-03 | |
Dissipation Factor? | 1MHz | ASTMD150 | 8E-03 | |
Dielectric Strength | | ASTMD149 | 17 | KV/mm |
Comparative Tracking Index | | ASTMD3638 | >600 | V |
High Voltage Arc Tracking Rate | HVTR | UL746 | 38.0 | mm/min |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Multi-Axial Instrumented Impact Energy | -40°C,能量to力量峰值 | ISO6603-2 | 23.0 | J |
Multi-Axial Instrumented Impact Energy | 23°C,能量to力量峰值 | ISO6603-2 | 19.0 | J |
Instrumented Dart Impact | -40°C,EnergyatPeakLoad | ASTMD3763 | 46.0 | J |
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 51.0 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | R-Scale | ASTMD785 | 117 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Transmittance | Total | ASTMD1003 | 81.0 | % |
Transmittance | Regular | ASTMD1003 | 77.0 | % |
Haze | | ASTMD1003 | 3.6 | % |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 1.6mm | UL94 | HB | |
UL flame retardant rating | 3.2mm | UL94 | V-2 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.