PC/PBT XENOY™ 1105-1001 SABIC INNOVATIVE SHANGHAI
108
- Unit Price:
- $2951 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 49MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Chemical resistance Low temperature impact re
- Application Areas:Electrical applications Household daily necessiti Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Specific volume | ASTMD792 | 1.20 | cm³/g | |
Melt mass flow rate | 250°C/5.0kg | ASTMD1238,ISO1133 | 16 | g/10min |
Shrinkage rate | MD:3.20mm | 内部方法 | 0.80到1.0 | % |
TD:3.20mm | 内部方法 | 0.80到1.0 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
--1 | ASTMD638 | 1990 | Mpa | |
--2 | ASTMD638 | 2020 | Mpa | |
Fracture 10 | ASTMD638 | 120 | % | |
crack | ISO527-2/50 | 120 | % | |
50.0mm span 11 | ASTMD790 | 1900 | Mpa | |
--12 | ISO178 | 2020 | Mpa | |
--13 | ISO178 | 78.9 | Mpa | |
Yield, 50.0mm span 14 | ASTMD790 | 76.1 | Mpa | |
Fracture, 50.0mm span 15 | ASTMD790 | 74.7 | Mpa | |
Fracture bending strain 16 | ISO178 | 7.3 | % | |
Surrender 3 | ASTMD638 | 45.2 | Mpa | |
Surrender 4 | ASTMD638 | 48.8 | Mpa | |
yield | ISO527-2/50 | 52.4 | Mpa | |
Fracture 5 | ASTMD638 | 46.0 | Mpa | |
Fracture 6 | ASTMD638 | 47.4 | Mpa | |
crack | ISO527-2/50 | 50.5 | Mpa | |
Surrender 7 | ASTMD638 | 4.1 | % | |
Surrender 8 | ASTMD638 | 4.2 | % | |
yield | ISO527-2/50 | 4.5 | % | |
Fracture 9 | ASTMD638 | 110 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
0.45MPa, unannealed, 64.0mm span 21 | ISO75-2/Bf | 109 | °C | |
1.8MPa, unannealed, 6.40mm | ASTMD648 | 97.0 | °C | |
1.8MPa, unannealed, 64.0mm span 22 | ISO75-2/Af | 90.2 | °C | |
Vicat softening temperature | ASTMD1525,ISO306/B50,ISO306/B12023 | 123 | °C | |
0.45MPa, unannealed, 6.40mm | ASTMD648 | 115 | °C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of simply supported beam gap 17 | -30°C | ISO179/1eA | 48 | kJ/m² |
23°C | ISO179/1eA | 63 | kJ/m² | |
-40°C | ASTMD256 | 370 | J/m | |
-30°C | ASTMD256 | 490 | J/m | |
-20°C | ASTMD256 | 690 | J/m | |
-10°C | ASTMD256 | 700 | J/m | |
0°C | ASTMD256 | 720 | J/m | |
23°C | ASTMD256 | 760 | J/m | |
-40°C18 | ISO180/1A | 35 | kJ/m² | |
-30°C19 | ISO180/1A | 51 | kJ/m² | |
23°C20 | ISO180/1A | 63 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore D | ISO868 | 79 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.