PCTA Eastar™ BR203 EASTMAN USA
200
- Unit Price:
- $3339 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 173MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility transparent
- Application Areas:packing food
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:3.20mm | ASTMD955 | 0.20to0.60 | % |
Density/specific gravity | ASTMD792 | 1.20 | g/cm³ | |
23°C | ISO1183 | 1.19 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strength | Yield,23°C | ASTMD638 | 46.0 | Mpa |
Break,23°C | ASTMD638 | 53.0 | Mpa | |
Tensile stress | Break,23°C | ISO527-2 | 49.0 | Mpa |
Yield,23°C | ISO527-2 | 47.0 | Mpa | |
Tensile strain | Break,23°C | ISO527-2 | 210 | % |
Yield,23°C | ISO527-2 | 4.0 | % | |
Bending stress | 23°C | ISO178 | 64.0 | Mpa |
elongation | Yield,23°C | ASTMD638 | 5.0 | % |
Break,23°C | ASTMD638 | 310 | % | |
Bending modulus | 23°C | ASTMD790 | 1900 | Mpa |
23°C | ISO178 | 1750 | Mpa | |
bending strength | Yield,23°C | ASTMD790 | 67.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO75-2/A | 66.0 | °C |
0.45MPa,Unannealed | ASTMD648 | 73.0 | °C | |
0.45MPa,Unannealed | ISO75-2/B | 73.0 | °C | |
1.8MPa,Unannealed | ASTMD648 | 65.0 | °C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Multi axis Instrumented Impact Energy | -40°C,能量to力量峰值 | ISO6603-2 | 55.0 | J |
23°C,能量to力量峰值 | ISO6603-2 | 71.0 | J | |
Dart impact equipped with measuring instruments | -40°C,EnergyatPeakLoad | ASTMD3763 | 48.0 | J |
23°C,EnergyatPeakLoad | ASTMD3763 | 45.0 | J | |
Impact strength of cantilever beam gap | -40°C | ASTMD4218 | NoBreak | |
23°C | ASTMD4218 | NoBreak | ||
-40°C | ASTMD256 | 60 | J/m | |
23°C | ASTMD256 | 370 | J/m | |
-40°C | ISO180 | 6.3 | kJ/m² | |
23°C | ISO180 | 30 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R-Sale,23°C | ASTMD785 | 105 |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Haze | ASTMD1003 | 0.30 | % | |
transmissivity | Regular | ASTMD1003 | 89.0 | % |
Total | ASTMD1003 | 91.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.