Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Moisture Absorption | Saturation,23°C,2.00mm | ISO62 | 0.70 | % |
Moisture Absorption | Equilibrium,23°C,2.00mm,50%RH | ISO62 | 0.20 | % |
Modeling Shrinkage | TD | ISO294-4 | 0.40 | % |
Modeling Shrinkage | MD | ISO294-4 | 0.20 | % |
Melt Volume flow Rate | 190°C/2.16kg | ISO1133 | 5.00 | cm3/10min |
MediumDensity | | | 1.02 | g/cm³ |
Melt Mass-Flow Rate | 190°C/2.16kg | ISO1133 | 5.3 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Creep Modulus | 1hr | ISO899-1 | 50.0 | Mpa |
Tensile Creep Modulus | 1000hr | ISO899-1 | 40.0 | Mpa |
Tensile Modulus | | ISO527-2 | 56.0 | Mpa |
Tensile Stress | 10%Strain | ISO527-2 | 4.10 | Mpa |
Tensile Stress | 50%Strain | ISO527-2 | 7.30 | Mpa |
Tensile Stress | Break | ISO527-2 | 26.0 | Mpa |
Tensile Stress | 5.0%Strain | ISO527-2 | 2.40 | Mpa |
Tensile Strain | Break | ISO527-2 | >300 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Linear thermal expansion coefficient | MD | ISO11359-2 | 2.2E-04 | cm/cm/°C |
Linear thermal expansion coefficient | TD | ISO11359-2 | 2.2E-04 | cm/cm/°C |
Melting Temperature | | ISO11357-3 | 150 | °C |
Glass Transition Temperature | | ISO11357-2 | -50.0 | °C |
Effective Thermal Diffusivity | | | 5.44E-08 | m²/s |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Relative Permittivity | 100Hz | IEC60250 | 5.20 | |
Relative Permittivity | 1MHz | IEC60250 | 4.70 | |
Comparative Tracking Index | | IEC60112 | 600 | V |
Dielectric Strength | | IEC60243-1 | 18 | KV/mm |
Dissipation Factor? | 100Hz | IEC60250 | 0.011 | |
Dissipation Factor? | 1MHz | IEC60250 | 0.053 | |
Surface Resistivity | | IEC60093 | 2E+14 | ohms |
Volume Resistivity | | IEC60093 | 7E+12 | ohms·cm |
Elastomers Properties | Test Condition | Test Method | Test Result | Unit |
---|
TearStrength-Flow | | ISO34-1 | 110 | kN/m |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Impact Strength | 23°C | ISO8256/1 | 230 | kJ/m² |
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | NoBreak | |
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | NoBreak | |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Shore Hardness | Shore D,15sec | ISO868 | 38 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 1.5mm | UL94 | HB | |
Oxygen Index | | ISO4589-2 | 20 | % |
FMVSS Flammability | | FMVSS302 | SE | |
Flammability level | 1.5mm | IEC60695-11-10,-20 | HB | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.