TPEE Arnitel® EL740-S DSM HOLAND
89
- Unit Price:
- $3156 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 30MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Low temperature resistanc High temperature resistan Thermal stability currency injection molding injection molding
- Application Areas:Cable Electric wire Automotive sector
- Color:--
- Grade:Injection grade
Technical Data Sheet
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Modulus | ISO 527 | 1000 | Mpa | |
Tensile Strength | ISO 527 | 38 | Mpa | |
hardness | ISO 868 | 72 | - | |
Notched Izod Impact Strength | 23℃ | ISO 180/1A | 9 | KJ/m |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melting temperature | ISO 11357 | 221 | °C | |
Deflection Temperature Under Load? | 0.45MPa | ISO 75 | 120 | °C |
Vicat Softening Temperature | ISO 306 | 160 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface Resistivity | IEC 60093 | 1E+15 | > | |
Volume Resistivity | IEC 60093 | 1E+13 | ||
Dielectric Strength | IEC 60243 | 23 | KV/mm | |
Dielectric Constant | IEC 60250 | 3.7 | - | |
Comparative Tracking Index | IEC 60112 | 600 | - |
Other | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hygroscopicity | ISO 62 | 0.15 | % |
Physical | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density / Specific Gravity | ISO 1183 | 1290 | kg/m | |
Moisture Absorption | ISO 62 | 0.6 | % | |
Melt index | ISO 1133 | 15 | g/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.