Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt index | 230℃/2.16 kg | ISO 1133 | 30 | g/10 min |
Modeling Shrinkage | | ISO 294-4 | 0.65 | % |
Moisture Absorption | 23℃, 24 hr | ISO 62 | 0.40 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
hardness | Shore D | ISO 868 | 55 | |
Flexural Modulus | | ISO 178 | 190 | Mpa |
Tensile Stress | Yield | ISO 527-2 | 40.0 | Mpa |
Tensile Strain | Break | ISO 527-2 | 500 | % |
Charpy Notched Impact Strength | | ISO 179/1eA | 无断裂 | |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45 MPa, Unannealed | ISO 75-2/B | 65.0 | °C |
Deflection Temperature Under Load? | 1.8 MPa, Unannealed | ISO 75-2/A | 45.0 | °C |
Melting temperature (DSC) | | ISO 3146 | 204 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface Resistivity | | IEC 60093 | 3.6E+13 | Ohm |
Volume Resistivity | | IEC 60093 | 2.1E+13 | ohm·cm |
Arc Resistance | 2.00 mm | IEC 60243-1 | 17 | KV/mm |
Physical | Test Condition | Test Method | Test Result | Unit |
---|
hardness | Shore D | ISO 868 | 55 | |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|
Tensile strength | | ISO 527 | 32 | Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.