Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:3.20mm | ASTMD955 | 0.20to0.60 | % |
Density / Specific Gravity | 23°C | ISO1183 | 1.19 | g/cm³ |
Density / Specific Gravity | | ASTMD792 | 1.20 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress | Break,23°C | ISO527-2 | 49.0 | Mpa |
Tensile Stress | Yield,23°C | ISO527-2 | 47.0 | Mpa |
Tensile Strain | Break,23°C | ISO527-2 | 210 | % |
Tensile Strain | Yield,23°C | ISO527-2 | 4.0 | % |
Tensile Strength | Yield,23°C | ASTMD638 | 46.0 | Mpa |
Tensile Strength | Break,23°C | ASTMD638 | 53.0 | Mpa |
Flexural Stress | 23°C | ISO178 | 64.0 | Mpa |
Tensile Elongation | Break,23°C | ASTMD638 | 310 | % |
Tensile Elongation | Yield,23°C | ASTMD638 | 5.0 | % |
Flexural Modulus | 23°C | ASTMD790 | 1900 | Mpa |
Flexural Modulus | 23°C | ISO178 | 1750 | Mpa |
Flexural Strength | Yield,23°C | ASTMD790 | 67.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ASTMD648 | 73.0 | °C |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 73.0 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 65.0 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 66.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface Resistivity | | ASTMD257 | 1E+17 | ohms |
Dielectric Constant | 23°C,1kHz | ASTMD150 | 2.60 | |
Dielectric Constant | 23°C,10kHz | ASTMD150 | 2.60 | |
Dielectric Constant | 23°C,100kHz | ASTMD150 | 2.50 | |
Dielectric Constant | 23°C,1MHz | ASTMD150 | 2.50 | |
Arc Resistance | | ASTMD495 | 123 | sec |
Volume Resistivity | 23°C | ASTMD257 | 1E+17 | ohms·cm |
Dielectric Strength | 23°C | ASTMD149 | 17 | KV/mm |
Dissipation Factor? | 23°C,1kHz | ASTMD150 | 6E-03 | |
Dissipation Factor? | 23°C,10kHz | ASTMD150 | 0.012 | |
Dissipation Factor? | 23°C,100kHz | ASTMD150 | 0.015 | |
Dissipation Factor? | 23°C,1MHz | ASTMD150 | 0.015 | |
Comparative Tracking Index | | ASTMD3638 | 700 | V |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod Impact Strength | -40°C | ASTMD256 | 60 | J/m |
Notched Izod Impact Strength | 23°C | ASTMD256 | 370 | J/m |
Notched Izod Impact Strength | -40°C | ISO180 | 6.3 | kJ/m² |
Notched Izod Impact Strength | 23°C | ISO180 | 30 | kJ/m² |
Notched Izod Impact Strength | -40°C | ASTMD4812 | NoBreak | |
Notched Izod Impact Strength | 23°C | ASTMD4812 | NoBreak | |
Multi-Axial Instrumented Impact Energy | -40°C,能量to力量峰值 | ISO6603-2 | 55.0 | J |
Multi-Axial Instrumented Impact Energy | 23°C,能量to力量峰值 | ISO6603-2 | 71.0 | J |
Instrumented Dart Impact | -40°C,EnergyatPeakLoad | ASTMD3763 | 48.0 | J |
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 45.0 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | R-Sale,23°C | ASTMD785 | 105 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Transmittance | Total | ASTMD1003 | 91.0 | % |
Transmittance | Regular | ASTMD1003 | 89.0 | % |
Haze | | ASTMD1003 | 0.30 | % |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Flame Rating | 3.0mm,AT | UL94 | V-2 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.