TPV Santoprene™ 251-80 P9H803 CELANESE USA
95
- Unit Price:
- $4580 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 30MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Dimensional stability Ozone resistant Chemical resistance
- Application Areas:Cable Cable sheath Wire and cable applicatio Application in the automo Automotive Applications Flexible cable sheath
- Color:--
- Grade:Extrusion grade
Technical Data Sheet
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
RTIElec | UL746 | 90.0 | °C | |
RTIStr | 1.5mm | UL746 | 85.0 | °C |
3.0mm | UL746 | 90.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Strength | 23°C,2.00mm | ASTMD149 | 28 | KV/mm |
Comparative Tracking Index | CTI | UL746 | PLC0 | |
High Amp Arc Ignition | HAI | UL746 | PLC0 | |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC2 | |
Hot-wire Ignition | HWI | UL746 | PLC3 | |
High Amp Arc Ignition | PLC | UL746 | PLC6 |
Elastomers Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress(Across Flow) | 100%Strain,23°C | ASTMD412 | 3.90 | Mpa |
100%Strain,23°C | ISO37 | 3.90 | Mpa | |
Tensile Strength (flow) | Break,23°C | ASTMD412 | 9.00 | Mpa |
Tensile Strength (TD) | Break,23°C | ISO37 | 9.00 | Mpa |
Tensile Elongation(Across Flow) | Break,23°C | ASTMD412 | 550 | % |
Break,23°C | ISO37 | 550 | % | |
Compression Set | 23°C,168hr | ASTMD395B | 31 | % |
70°C,22hr | ASTMD395B | 40 | % | |
100°C,168hr | ASTMD395B | 55 | % | |
Compression Set | 23°C,168hr | ISO815 | 31 | % |
70°C,22hr | ISO815 | 40 | % | |
100°C,168hr | ISO815 | 55 | % |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore Hardness | Shore A,15sec,23°C | ISO868 | 86 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.5mm | UL94 | V-0 | |
3.0mm | UL94 | V-0 | ||
Oxygen Index | ASTMD2863 | 27 | % | |
ISO4589-2 | 27 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.