TPV 3170N DSM HOLAND
82
- Unit Price:
- $3496 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:--
Technical Data Sheet
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
RTIElec | UL746 | 50.0 | °C | |
Evolution Calendar intelligent importer | UL746 | 50.0 | °C | |
RTIStr | UL746 | 50.0 | °C |
Aging Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Change in Durometer Hardness in Air | Shore A,135°C,1000hr | ASTMD573 | -1.0 | |
Shore A,150°C,168hr | ASTMD573 | 3.0 | ||
Change in Shore Hardness in Air | Shore A,135°C,1000hr | ISO188 | -1.0 | |
Shore A,150°C,168hr | ISO188 | 3.0 | ||
Change in Volume | 125°C,70hr,在IRM903油中 | ASTMD471 | 120 | % |
125°C,70hr,在IRM903油中 | ISO1817 | 120 | % | |
Change in Tensile Strength in Air(Across Flow) | 135°C,1000hr | ASTMD573 | -8.0 | % |
100%Strain,135°C,1000hr | ASTMD573 | 10 | % | |
150°C,168hr | ASTMD573 | -4.0 | % | |
100%Strain,150°C,168hr | ASTMD573 | 5.0 | % | |
135°C,1000hr | ISO188 | -8.0 | % | |
100%Strain135°C,1000hr | ISO188 | 10 | % | |
150°C,168hr | ISO188 | -4.0 | % | |
100%Strain150°C,168hr | ISO188 | 5.0 | % | |
Change in Tensile Strain at Break in Air?(Flow) | 135°C,1000hr | ISO188 | -13 | % |
150°C,168hr | ISO188 | -14 | % | |
Change in Ultimate Elongation in Air (Flow) | 135°C,1000hr | ASTMD573 | -13 | % |
150°C,168hr | ASTMD573 | -14 | % |
Elastomers Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tearing Strength (MD) | ASTMD624 | 42.0 | kN/m | |
Tearing Strength (MD) | ISO34-1 | 42 | kN/m | |
Tensile Stress | Break | ISO37 | 7.70 | Mpa |
Across Flow:100%Strain | ASTMD412 | 3.30 | Mpa | |
流量:100%Strain | ASTMD412 | 5.10 | Mpa | |
Across Flow:100%Strain | ISO37 | 3.30 | Mpa | |
流量:100%Strain | ISO37 | 5.10 | Mpa | |
流量:Break | ISO37 | 6.70 | Mpa | |
Tensile Strength | Break | ASTMD412 | 7.72 | Mpa |
流量:Break | ASTMD412 | 6.70 | Mpa | |
Tensile Elongation | Break | ASTMD412 | 670 | % |
流量:Break | ASTMD412 | 300 | % | |
Break | ISO37 | 670 | % | |
流量:Break | ISO37 | 300 | % | |
Compression Set | 23°C,22hr | ASTMD395 | 25 | % |
70°C,22hr | ASTMD395 | 43 | % | |
125°C,70hr | ASTMD395 | 63 | % | |
23°C,22hr | ISO815 | 25 | % | |
70°C,22hr | ISO815 | 43 | % | |
125°C,70hr | ISO815 | 63 | % |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore Hardness | Shore A,5sec,挤塑 | ASTMD2240 | 71 | |
Shore A,5sec,Injection | ASTMD2240 | 75 | ||
Shore A,5sec,挤塑 | ISO868 | 71 | ||
Shore A,5sec,Injection | ISO868 | 75 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flame Rating | 1.5mm,NaturalandBlackColors | UL94 | HB |
Supplementary information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
ApparentShearViscosity-Capillary,@206/s | 200°C | ISO11443 | 290 | Pa·s |
200°C | ASTMD3835 | 290 | Pa·s |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.