Need Help? Contact Us service@plas.com
Get App

TPV Santoprene™ 8201-60 CELANESE USA

88
  • Unit Price:
    $4015 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    30MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Low friction coefficient Low mold expansion Recyclable materials Controllable mold expansi Cleanable Good melt strength Good colorability Ozone resistance Chemical resistance Low water absorption Not absorbing water
  • Application Areas:Kitchen utensils Home appliance components Fatigue relief supplies Soft handle Stationery Smart phone Kitchen utensils Home appliance components Fatigue relief supplies Soft handle Phone Stationery
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Brittleness TemperatureASTMD746-60.0°C
Brittleness TemperatureISO812-60.0°C
RTIElecUL746100°C
RTIStr1.1mmUL74690.0°C
RTIStr1.6mmUL74690.0°C
RTIStr3.0mmUL74695.0°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
Comparative Tracking IndexCTIUL746PLC0
Hot-wire Ignition1.6mmUL746PLC3
Hot-wire Ignition3.0mmUL746PLC2
High Amp Arc IgnitionHAIUL746PLC0
High Amp Arc IgnitionPLCUL746PLC5
Aging PropertiesTest ConditionTest MethodTest ResultUnit
Change in Durometer Hardness in AirShoreA,150°C,168hrASTMD5731.0
Change in Shore Hardness in AirShoreA,150°C,168hrISO1881.0
ChangeinMassinAir150°C,168hrASTMD573-8.0%
ChangeinMassinAir150°C,168hrISO188-8.0%
Tensile Stress(Break)23°C,168hr,inIRM903OilISO1817-21%
Tensile Stress(Break)23°C,168hr,inSodiumChloride,15%ISO1817-5.0%
Tensile Stress(Break)23°C,168hr,inSodiumHydroxide,50%ISO1817-2.0%
Tensile Stress(Break)23°C,168hr,inSulfuricAcid,98%ISO18175.0%
Tensile Stress(Break)23°C,168hr,在水中ISO181711%
Change in Ultimate Elongation in Air150°C,168hrASTMD573-7.0%
Change in Durometer HardnessShoreA,23°C,168hr,inIRM903OilASTMD471-13
Change in Durometer HardnessShoreA,23°C,168hr,inSodiumChloride,15%ASTMD4712.0
Change in Durometer HardnessShoreA,23°C,168hr,inSodiumHydroxide,50%ASTMD4712.0
Change in Durometer HardnessShoreA,23°C,168hr,inSulfuricAcid,98%ASTMD471-1.0
Change in Durometer HardnessShoreA,23°C,168hr,inWaterASTMD4710.0
ChangeinShoreHardnessShoreA,23°C,168hr,inIRM903OilISO1817-13
ChangeinShoreHardnessShoreA,23°C,168hr,inSodiumChloride,15%ISO18172.0
ChangeinShoreHardnessShoreA,23°C,168hr,inSodiumHydroxide,50%ISO18172.0
ChangeinShoreHardnessShoreA,23°C,168hr,inSulfuricAcid,98%ISO1817-1.0
ChangeinShoreHardnessShoreA,23°C,168hr,inWaterISO18170.0
Change in Ultimate Elongation23°C,168hr,inSodiumHydroxide,50%ASTMD471-2.0%
Change in Ultimate Elongation23°C,168hr,inSulfuricAcid,98%ASTMD4715.0%
Change in Ultimate Elongation23°C,168hr,在水中ASTMD47111%
Change in Ultimate Elongation23°C,168hr,inIRM903OilASTMD471-21%
Change in Ultimate Elongation23°C,168hr,inSodiumChloride,15%ASTMD471-5.0%
Change in Tensile Strength23°C,168hr,inIRM903OilASTMD471-17%
Change in Tensile Strength23°C,168hr,inSodiumChloride,15%ASTMD471-4.0%
Change in Tensile Strength23°C,168hr,inSodiumHydroxide,50%ASTMD471-2.0%
Change in Tensile Strength23°C,168hr,inSulfuricAcid,98%ASTMD4713.0%
Change in Tensile Strength23°C,168hr,在水中ASTMD471-3.0%
Change in Tensile Strength23°C,168hr,inIRM903OilISO1817-17%
Change in Tensile Strength23°C,168hr,inSodiumChloride,15%ISO1817-4.0%
Change in Tensile Strength23°C,168hr,inSodiumHydroxide,50%ISO1817-2.0%
Change in Tensile Strength23°C,168hr,inSulfuricAcid,98%ISO18173.0%
Change in Tensile Strength23°C,168hr,在水中ISO1817-3.0%
Change in Tensile Strength in Air150°C,168hrASTMD573-9.0%
Change in Tensile Strength in Air150°C,168hrISO188-9.0%
Change in Mass23°C,168hr,inIRM903OilASTMD47147%
Change in Mass23°C,168hr,inSodiumChloride,15%ASTMD4710.0%
Change in Mass23°C,168hr,inSodiumHydroxide,50%ASTMD4710.0%
Change in Mass23°C,168hr,inSulfuricAcid,98%ASTMD4710.0%
Change in Mass23°C,168hr,在水中ASTMD4710.0%
Change in Mass23.0°C,168hr,inSodiumHydroxide,50%ISO18170.0%
Change in Mass23.0°C,168hr,inSulfuricAcid,98%ISO18170.0%
Change in Mass23.0°C,168hr,inSodiumChloride,15%ISO18170.0%
Change in Mass23.0°C,168hr,inIRM903OilISO181747%
Elastomers PropertiesTest ConditionTest MethodTest ResultUnit
Tearing Strength (MD)23°CASTMD62432.0kN/m
Compression Set70°C,22hrISO81529%
TearStrength-AcrossFlow323°CISO34-132kN/m
Compression Set70°C,22hrASTMD395B29%
Tensile Stress(Across Flow)100%Strain,23°CASTMD4122.20Mpa
Tensile Stress(Across Flow)100%Strain,23°CISO372.20Mpa
Tensile Strength (flow)Break,23°CASTMD4125.90Mpa
Tensile Strength (TD)Break,23°CISO375.90Mpa
Tensile Elongation(Across Flow)Break,23°CASTMD412520%
Tensile Elongation(Across Flow)Break,23°CISO37520%
hardnessTest ConditionTest MethodTest ResultUnit
Shore HardnessShore A,15sec,23°CISO86864
FlammabilityTest ConditionTest MethodTest ResultUnit
UL flame retardant rating1.1mmUL94HB
UL flame retardant rating1.6mmUL94HB
UL flame retardant rating3.0mmUL94HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.