PSU UDEL® P-3500 BK SOLVAY USA
179
- Unit Price:
- $13838 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Hydrolysis resistance Chemical resistance
- Application Areas:Industrial components Home appliance components
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD | ASTMD955 | 0.70 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.30 | % |
Melt Mass-Flow Rate | 343°C/2.16kg | ASTMD1238 | 3.0to5.0 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Modulus | ASTMD638 | 2480 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 50to100 | % |
Flexural Modulus | ASTMD790 | 2690 | Mpa | |
Flexural Strength | ASTMD790 | 106 | Mpa | |
Tensile Strength | Break | ASTMD638 | 70.3 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 174 | °C |
Linear thermal expansion coefficient | MD | ASTMD696 | 5.6E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Strength | ASTMD149 | 17 | KV/mm | |
Dissipation Factor? | 60Hz | ASTMD150 | 7E-03 | |
1kHz | ASTMD150 | 1E-03 | ||
1MHz | ASTMD150 | 6E-03 | ||
Dielectric Constant | 1kHz | ASTMD150 | 3.04 | |
1MHz | ASTMD150 | 3.02 | ||
60Hz | ASTMD150 | 3.03 | ||
Volume Resistivity | ASTMD257 | 3E+16 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Impact Strength | ASTMD1822 | 420 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.