Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD | ASTMD955 | 0.40到0.60 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Strength | Yield | ASTMD638 | 83.0 | Mpa |
Tensile Strength | Break | ASTMD638 | 69.0 | Mpa |
Tensile Modulus | | ASTMD638 | 1900 | Mpa |
Tensile Elongation | Yield | ASTMD638 | 9.0 | % |
Tensile Elongation | Break | ASTMD638 | 30 | % |
Flexural Modulus | | ASTMD790 | 2300 | Mpa |
Flexural Strength | | ASTMD790 | 97.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ASTMD648 | 132 | °C |
Deflection Temperature Under Load? | 0.45MPa,Annealed | ASTMD648 | 143 | °C |
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ASTMD648 | 116 | °C |
Deflection Temperature Under Load? | 1.8MPa,Annealed | ASTMD648 | 138 | °C |
Vicat Softening Temperature | | ASTMD1525 | 147 | °C |
Linear thermal expansion coefficient | MD | ASTMD696 | 5.8E-05 | cm/cm/°C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Instrumented Dart Impact | 23°C,TotalEnergy | ASTMD3763 | 68.0 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell Hardness | M-Scale | ASTMD785 | 92 | |
Rockwell Hardness | R-Scale | ASTMD785 | 124 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Transmittance | | ASTMD1003 | 88.0 | % |
The Yellow Index | | ASTMD1925 | 40 | YI |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.