Technical Data Sheet
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Taber Abrasion Resistance | 1000Cycles,1000g,H-18Wheel | ASTMD3389 | 34.0 | mg |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Glass Transition Temperature | | ASTMD3418 | -25.0 | °C |
Melting temperature | | DSC | 120 | °C |
Kofler Melting Temperature | | 内部方法 | 115 | °C |
Elastomers Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Set | 200%Strain | ASTMD412 | 13 | % |
Tensile Stress | 100%Strain,0.762mm | ASTMD412 | 5.50 | Mpa |
Tensile Stress | 300%Strain,0.762mm | ASTMD412 | 9.70 | Mpa |
Tensile Strength | Break,0.762mm | ASTMD412 | 51.7 | Mpa |
Tensile Elongation | Break,0.762mm | ASTMD412 | 540 | % |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Shore Hardness | Shore A | ASTMD2240 | 85 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Haze | 1650µm | ASTMD1003 | 1.1 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.