ASA GELOY™ HRA222-WH4C030U SABIC INNOVATIVE US
101
- Unit Price:
- $3805 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 40MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:UV resistance Flame retardant
- Application Areas:Electrical field Electrical appliances Electronic field
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Moisture Absorption | 饱和,23°C | ISO62 | 0.60 | % |
平衡,23°C,50%RH | ISO62 | 0.20 | % | |
Melt Volume flow Rate | 260°C/2.16kg | ISO1133 | 13.0 | cm3/10min |
Density | ISO1183 | 1.17 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | 断裂 | ISO527-2/50 | 45.0 | Mpa |
Tensile Strain | 断裂 | ISO527-2/5 | >50 | % |
断裂 | ISO527-2/50 | >50 | % | |
Tensile Strength | 屈服 | ASTMD638 | 63.0 | Mpa |
断裂 | ASTMD638 | 56.0 | Mpa | |
Tensile Modulus | ISO527-2/1 | 2520 | Mpa | |
Tensile Elongation | 屈服 | ASTMD638 | 4.3 | % |
断裂3 | ASTMD638 | >100 | % | |
断裂2 | ASTMD638 | >100 | % | |
屈服 | ASTMD638 | 4.2 | % | |
Flexural Modulus | ISO178 | 2520 | Mpa | |
Flexural Strength | ISO178 | 93.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,100mmSpan | ISO75-2/Be | 99.0 | °C |
1.8MPa,Unannealed,100mmSpan | ISO75-2/Ae | 88.0 | °C | |
Vicat Softening Temperature | -- | ISO306/A50 | 111 | °C |
-- | ISO306/B50 | 102 | °C | |
-- | ISO306/B120 | 104 | °C | |
Linear thermal expansion coefficient | MD:-30到80°C | ISO11359-2 | 6.9E-05 | cm/cm/°C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Notched Izod Impact Strength | -30°C | ISO180/1A | 9.0 | kJ/m² |
0°C | ISO180/1A | 12 | kJ/m² | |
23°C | ISO180/1A | 17 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.