Material Description
Technical Data Sheet
Material Description
- Material Properties:Weather resistance UV resistance
- Application Areas:Lawn and garden equipment Electrical tools Electrical field Electrical appliances Electronic field sheet Automotive sector Lighting fixtures
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | ISO294-4 | 0.50到0.90 | % | |
Moisture Absorption | Saturation,23°C | ISO62 | 1.7 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.35 | % | |
Melt Volume flow Rate | 220°C/10.0kg | ISO1133 | 4.00 | cm3/10min |
Apparent Density | 0.59 | g/cm³ | ||
Density / Specific Gravity | ISO1183 | 1.07 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Stress | ISO178 | 65.0 | Mpa | |
Tensile Stress | Yield,23°C | ISO527-2 | 47.0 | Mpa |
Tensile Strain | Yield,23°C | ISO527-2 | 3.3 | % |
Tensile Creep Modulus | 1hr | ISO899-1 | 2000 | Mpa |
1000hr | ISO899-1 | 1200 | Mpa | |
Tensile Modulus | ISO527-2 | 2200 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat Softening Temperature | -- | ISO306/A50 | 104 | °C |
-- | ISO306/B50 | 92.0 | °C | |
Linear thermal expansion coefficient | MD | ISO11359-2 | 8.0E-5到1.1E-4 | cm/cm/°C |
Thermal Conductivity | DIN52612 | 0.17 | W/m/K | |
Heat Deflection Temperature | 0.45MPa,Annealed | ISO75-2/B | 101 | °C |
1.8MPa,Annealed | ISO75-2/A | 96.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation Factor? | 100Hz | IEC60250 | 9E-03 | |
1MHz | IEC60250 | 0.034 | ||
Surface Resistivity | IEC60093 | 1E+13 | ohms | |
Dielectric Constant | 100Hz | IEC60250 | 3.80 | |
Volume Resistivity | IEC60093 | 1E+14 | ohms·cm |
Film | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Elongation - MD | Break | ISO527-3 | 12 | % |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179 | 4.0 | kJ/m² |
23°C | ISO179 | 30 | kJ/m² | |
Notched Izod Impact Strength | -30°C | ISO180/A | 4.0 | kJ/m² |
23°C | ISO180/A | 15 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Ball Indentation Hardness | ISO2039-1 | 70.0 | Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.