Need Help? Contact Us service@plas.com
Get App

MVLDPE Exceed™  1018CA EXXONMOBIL USA

47
  • Unit Price:
    $1261 USD/MT
  • Packaging Specification:
    25KG/PKG
  • Supply Quantity:
    20MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Melt Mass-Flow Rate190°C/2.16kgASTMD12381.0g/10min
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Elmendorf Tear StrengthMDASTM D-1922280g
Elmendorf Tear StrengthTDASTM D-1922460g
Tensile Elongation (Break TD)@厚 150μ(5.9mil)ASTM D-882700%
Tensile Elongation (Break MD)@厚 150μ(5.9mil)ASTM D-882500%
Instrumented Dart ImpactF50ASTM D-1709A560g
Tensile Strength (Yield MD)@厚 150μ(5.9mil)ASTM D-8829Mpa
Tensile Strength (Yield TD)@厚 150μ(5.9mil)ASTM D-8829.7Mpa
Tensile Strength (Yield)@厚 150μ(5.9mil)ASTM D-88275.8Mpa
Tensile Strength (Break TD)@厚 150μ(5.9mil)ASTM D-88262.7Mpa
Flexural Modulus - 1% Secant@厚 150μ(5.9mil)ASTM D-882183Mpa
1%正割模量(TD)@厚 150μ(5.9mil)ASTM D-882205Mpa
Film Puncture ForceExxonMobil Method4.3J
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Melt TemperatureExxonMobil Method119°C
FilmTest ConditionTest MethodTest ResultUnit
Tensile Strength (TD)YieldASTMD8829.40Mpa
Tensile Strain (TD)BreakASTMD882600%
Elmendorf Tear Strength (MD)ASTMD1922250g
Elmendorf Tear Strength (TD)ASTMD1922470g
Gardner ImpactASTMD1709A460g
Tensile Strength (TD)BreakASTMD88242.7Mpa
Secant Modulus (1%Secant,MD)ASTMD882185Mpa
Secant Modulus (1%Secant,TD)ASTMD882192Mpa
Tensile Strength-MDYieldASTMD8829.37Mpa
Tensile Strength-MDBreakASTMD88254.3Mpa
Elongation - MDBreakASTMD882500%
OtherTest ConditionTest MethodTest ResultUnit
PPA
anti-sticking agent
slip additive
heat stabilizer
optical performance Test ConditionTest MethodTest ResultUnit
GlossAcross Flow,45°ASTM D-245742
Gloss45°ASTMD245739
HazeASTMD100318%
HazeASTM D-100318%
PhysicalTest ConditionTest MethodTest ResultUnit
DensityExxonMobil Method0.918g/cm³
Melt Mass-Flow RateASTM D-12381g/10min
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.