Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | TD | ISO294-4 | 1.2 | % |
Modeling Shrinkage | MD | ISO294-4 | 1.8 | % |
Moisture Absorption | Equilibrium,23°C,2.00mm,50%RH | ISO62 | 1.2 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress | Yield | ISO527-2 | 40.0 | Mpa |
Tensile Strain | Yield | ISO527-2 | 5.5 | % |
Nominal Tensile Strain at Break | | ISO527-2 | >50 | % |
Tensile Modulus | | ISO527-2 | 1500 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed | ISO75-2/A | 50.0 | °C |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 100 | °C |
Melting Temperature | | ISO11357-3 | 223 | °C |
Glass Transition Temperature | | ISO11357-2 | 60.0 | °C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | NoBreak | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
FMVSS Flammability | | FMVSS302 | B | |
Burning Rate | 1.00mm | ISO3795 | <100 | mm/min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.