PA610 LNP™ LUBRICOMP™ QL4040 NT92 SABIC INNOVATIVE US
161
- Unit Price:
- $5589 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability Conductive Glass fiber reinforced
- Application Areas:Electrical tools Electronic and Electrical
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:24hr | ASTMD955 | 1.0to3.0 | % |
TD:24hr | ASTMD955 | 1.0to3.0 | % | |
Moisture Absorption | 24hr,50%RH | ASTMD570 | 0.26 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.37 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Yield | ISO527-2/5 | 53.0 | Mpa |
Break | ISO527-2/5 | 52.0 | Mpa | |
Tensile Strain | Yield | ISO527-2/5 | 11 | % |
Break | ISO527-2/5 | 11 | % | |
Tensile Modulus | ISO527-2/1 | 2490 | Mpa | |
Flexural Stress | ISO178 | 50.0 | Mpa | |
Tensile Elongation | Yield | ASTMD638 | 14 | % |
Tensile Modulus | ASTMD638 | 2430 | Mpa | |
Tensile Strength | Break | ASTMD638 | 53.0 | Mpa |
Yield | ASTMD638 | 53.0 | Mpa | |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 1710 | Mpa |
Tensile Elongation | Break | ASTMD638 | 16 | % |
Flexural Modulus | ISO178 | 2320 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Heat Deflection Temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 60.0 | °C |
0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 170 | °C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 181 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 56.0 | °C | |
Linear thermal expansion coefficient | TD:-30to30°C | ASTMD696 | 1.1E-04 | cm/cm/°C |
MD:-30to30°C | ASTMD696 | 1.1E-04 | cm/cm/°C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Multi-Axial Instrumented Impact Energy | ISO6603-2 | 1.40 | J | |
Instrumented Dart Impact | 23°C,TotalEnergy | ASTMD3763 | 3.20 | J |
Notched Izod Impact Strength | 23°C | ISO180/1A | 4.2 | kJ/m² |
Unnotched Izod Impact Strength | 23°C | ISO180/1U | 32 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.