PA610 LNP™ LUBRICOMP™ QFL-4036 SABIC INNOVATIVE US
213
- Unit Price:
- $5893 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 20MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability Conductive Glass fiber reinforced
- Application Areas:Electrical tools Electronic and Electrical
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:24hr | ASTMD955 | 0.20 | % |
TD:24hr | ASTMD955 | 0.70 | % | |
TD:24hr | ISO294-4 | 0.70 | % | |
MD:24hr | ISO294-4 | 0.17 | % | |
Moisture Absorption | 24hr,50%RH | ASTMD570 | 0.14 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.22 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Modulus | --3 | ASTMD638 | 11000 | Mpa |
-- | ISO527-2/1 | 9800 | Mpa | |
Tensile Elongation | Break | ASTMD638,ISO527-2 | 2.6 | % |
Flexural Modulus | -- | ASTMD790 | 8480 | Mpa |
-- | ISO178 | 9700 | Mpa | |
Flexural Strength | -- | ASTMD790 | 221 | Mpa |
-- | ISO178 | 228 | Mpa | |
Coefficient of Friction | Dynamic | ASTMD3702Modified | 0.71 | |
Static | ASTMD3702Modified | 0.52 | ||
Tensile Strength | Break | ASTMD638 | 149 | Mpa |
Break | ISO527-2 | 150 | Mpa | |
Specific Wear Rate | ASTMD3702Modified | 15.0 | 10^-10in^5-min/ft-lb-hr |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 224 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 216 | °C | |
1.8MPa,Unannealed,64.0mmSpan5 | ISO75-2/Af | 211 | °C | |
Linear thermal expansion coefficient | MD:-40to40°C | ASTME831,ISO11359-2 | 2.9E-05 | cm/cm/°C |
TD:-40to40°C | ASTME831 | 7.4E-05 | cm/cm/°C | |
TD:-40to40°C | ISO11359-2 | 7.5E-05 | cm/cm/°C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Unnotched Izod Impact Strength | 23°C | ASTMD4812 | 940 | J/m |
23°C4 | ISO180/1U | 65 | kJ/m² | |
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 8.50 | J |
-- | ISO6603-2 | 3.19 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.