Need Help? Contact Us service@plas.com
Get App

PES LNP™ THERMOCOMP™  JF1006 BK81565 SABIC INNOVATIVE US

44
  • Unit Price:
    $36373 USD/MT
  • Packaging Specification:
    25KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageMD:24hrASTMD9550.30%
Modeling ShrinkageTD:24hrASTMD9550.50%
Modeling ShrinkageTD:24hrISO294-40.48%
Modeling ShrinkageMD:24hrISO294-40.27%
Moisture Absorption24hr,50%RHASTMD5700.34%
Moisture AbsorptionEquilibrium,23°C,50%RHISO620.46%
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile StressBreakISO527-2136Mpa
Tensile StrainBreakISO527-22.1%
Tensile ModulusISO527-2/19450Mpa
Tensile ElongationBreakASTMD6382.2%
Flexural ModulusASTMD7909720Mpa
Flexural ModulusISO17810000Mpa
Flexural StrengthASTMD790210Mpa
Flexural StressISO178208Mpa
Coefficient of FrictionDynamicASTMD3702Modified0.52
Coefficient of FrictionStaticASTMD3702Modified0.57
Tensile ModulusASTMD63810800Mpa
Tensile StrengthBreakASTMD638143Mpa
Specific Wear RateASTMD3702Modified17010^-10in^5-min/ft-lb-hr
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Heat Deflection Temperature1.8MPa,Unannealed,64.0mmSpanISO75-2/Af210°C
Deflection Temperature Under Load?1.8MPa,Unannealed,3.20mmASTMD648210°C
Linear thermal expansion coefficientMD:-40to40°CASTME8313.1E-05cm/cm/°C
Linear thermal expansion coefficientMD:-40to40°CISO11359-23.1E-05cm/cm/°C
Linear thermal expansion coefficientTD:-40to40°CASTME8313.6E-05cm/cm/°C
Linear thermal expansion coefficientTD:-40to40°CISO11359-23.7E-05cm/cm/°C
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Multi-Axial Instrumented Impact EnergyISO6603-24.16J
Notched Izod Impact Strength23°CISO180/1A9.5kJ/m²
UnnotchedIzodImpactStrength323°CISO180/1U40kJ/m²
Instrumented Dart Impact23°C,EnergyatPeakLoadASTMD376310.7J
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.