PEI LNP™ THERMOCOMP™ EC-1005 EM(EE005E-BK1A604) SABIC INNOVATIVE US
64
- Unit Price:
- $16044 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant Carbon fiber reinforced
- Application Areas:Automotive components Communication equipment
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:24hr | ASTMD955 | 0.070to0.090 | % |
TD:24hr | ASTMD955 | 0.50to0.70 | % | |
TD:24hr | ISO294-4 | 0.30to0.50 | % | |
MD:24hr | ISO294-4 | 0.10to0.30 | % | |
Moisture Absorption | 24hr,50%RH | ASTMD570 | 0.17 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.27 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Break | ISO527-2/5 | 200 | Mpa |
Tensile Strain | Break | ISO527-2/5 | 1.4 | % |
Tensile Modulus | ISO527-2/1 | 18200 | Mpa | |
Tensile Modulus | ASTMD638 | 18300 | Mpa | |
Tensile Strength | Break | ASTMD638 | 200 | Mpa |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 16300 | Mpa |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 275 | Mpa |
Tensile Elongation | Break | ASTMD638 | 1.4 | % |
Flexural Modulus | ISO178 | 16200 | Mpa | |
Flexural Strength | Break,50.0mmSpan | ASTMD790 | 274 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Heat Deflection Temperature | 0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 212 | °C |
1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 207 | °C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 210 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 204 | °C | |
Linear thermal expansion coefficient | MD:-30to30°C | ASTMD696 | 2.1E-05 | cm/cm/°C |
MD:-40to40°C | ASTME831 | 1.9E-05 | cm/cm/°C | |
MD:-40to40°C | ISO11359-2 | 1.9E-05 | cm/cm/°C | |
TD:-30to30°C | ASTMD696 | 2.7E-05 | cm/cm/°C | |
TD:-40to40°C | ASTME831 | 2.7E-05 | cm/cm/°C | |
TD:-40to40°C | ISO11359-2 | 2.7E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface Resistivity | ASTMD257 | 1.0E+2to1.0E+5 | ohms | |
Volume Resistivity | ASTMD257 | 1.0E+2to1.0E+6 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 10.4 | J |
23°C,TotalEnergy | ASTMD3763 | 11.6 | J | |
Multi-Axial Instrumented Impact Energy | ISO6603-2 | 3.00 | J | |
Unnotched Izod Impact Strength | 23°C | ISO180/1U | 24 | kJ/m² |
Notched Izod Impact Strength | 23°C | ISO180/1A | 4.8 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.