Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.87to0.92 | % |
Moisture Absorption | Saturation,23°C | ISO62 | 0.76 | % |
Melt Mass-Flow Rate | 295°C/6.6kg | ASTMD1238 | 7.0 | g/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17Wheel | ASTMD1044 | 50.0 | mg |
Tensile Elongation | Break | ASTMD638 | 20 | % |
Tensile Elongation | Yield | ASTMD638 | 5.0 | % |
Tensile Modulus | | ASTMD638 | 2400 | Mpa |
Tensile Strength | Break | ASTMD638 | 53.0 | Mpa |
Tensile Strength | Yield | ASTMD638 | 62.0 | Mpa |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 94.0 | Mpa |
Flexural Modulus | | ISO178 | 2000 | Mpa |
Flexural Strength | | ISO178 | 98.0 | Mpa |
Tensile Stress | Yield | ISO527-2/50 | 68.0 | Mpa |
Tensile Stress | Break | ISO527-2/50 | 59.0 | Mpa |
Tensile Strain | Yield | ISO527-2/50 | 5.0 | % |
Tensile Strain | Break | ISO527-2/50 | 15 | % |
Tensile Modulus | | ISO527-2/1 | 2300 | Mpa |
Flexural Modulus | -- | ASTMD790 | 2150 | Mpa |
Flexural Modulus | 50.0mmSpan4 | ASTMD790 | 2150 | Mpa |
Flexural Strength | | ASTMD790 | 94.0 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed,3.20mm | ASTMD648 | 145 | °C |
Heat Deflection Temperature | 0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 164 | °C |
Vicat Softening Temperature | | ISO306/B120 | 180 | °C |
Glass Transition Temperature | | DSC | 200 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface Resistivity | | ASTMD257 | >1.0E+15 | ohms |
Dielectric Constant | 100Hz | ASTMD150 | 3.13 | |
Dielectric Constant | 100kHz | ASTMD150 | 3.07 | |
Dielectric Constant | 1MHz | ASTMD150 | 3.04 | |
Volume Resistivity | | ASTMD257 | >1.0E+16 | ohms·cm |
Dissipation Factor? | 1MHz | ASTMD150 | 5.4E-03 | |
Dissipation Factor? | 100Hz | ASTMD150 | 0.011 | |
Dissipation Factor? | 100kHz | ASTMD150 | 6.1E-03 | |
Dielectric Strength | 3.20mm,inOil | ASTMD149 | 17 | KV/mm |
Elastomers Properties | Test Condition | Test Method | Test Result | Unit |
---|
TearStrength7 | 1.60mm | ISO34-1 | 37 | kN/m |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Notched Izod Impact Strength | -30°C | ISO180/1A | 8.0 | kJ/m² |
Notched Izod Impact Strength | 23°C | ISO180/1A | 16 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Shore Hardness | Shore D | ASTMD2240 | 80 | |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|
Oxygen Index | | ASTMD2863 | 48 | % |
UL flame retardant rating | 1.6mm,TestingbySABIC | UL94 | V-0 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.