PEI ULTEM™ 4000-7401 SABIC INNOVATIVE US
115
- Unit Price:
- $13601 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 26.1MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High temperature resistan enhance
- Application Areas:Electrical tools Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.20to0.30 | % |
Moisture Absorption | 24hr | ASTMD570 | 0.11 | % |
Melt Mass-Flow Rate | 337°C/6.6kg | ASTMD1238 | 3.1 | g/10min |
K (wear) Factor | --2 | 内部方法 | 62.0 | |
--3 | 内部方法 | 1900 | ||
PVLimit4 | 内部方法 | 2.1 | MPa·m/s |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17Wheel | ASTMD1044 | 33.0 | mg |
Coefficient of Friction | Steel - Dynamic | ASTMD1894 | 0.24 | |
Steel - Static6 | ASTMD1894 | 0.25 | ||
Flexural Modulus | 100mmSpan | ASTMD790 | 8830 | Mpa |
Tensile Strain | Break | ASTMD638 | 1.2 | % |
Flexural Strength | Yield,100mmSpan | ASTMD790 | 114 | Mpa |
Break,100mmSpan | ASTMD790 | 138 | Mpa | |
Tensile Strength | Break | ASTMD638 | 82.7 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8MPa,Unannealed,6.40mm | ASTMD648 | 212 | °C |
Vicat Softening Temperature | ASTMD15257 | 234 | °C | |
RTIElec | UL746 | 105 | °C | |
Evolution Calendar intelligent importer | UL746 | 105 | °C | |
RTIStr | UL746 | 105 | °C | |
Linear thermal expansion coefficient | MD:-40to40°C | ASTME831 | 1.6E-05 | cm/cm/°C |
MD:-20to150°C | ASTME831 | 1.6E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Comparative Tracking Index | CTI | UL746 | PLC4 |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Reverse Notch Izod Impact | 3.20mm | ASTMD256 | 170 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | M-Scale | ASTMD785 | 85 |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.8mm | UL94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.