PEI ULTEM™ 4001-7402 SABIC INNOVATIVE US
188
- Unit Price:
- $11037 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 69.5MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:wear resistant enhance
- Application Areas:Aerospace Applications Automotive sector
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:3.20mm | 内部方法 | 0.50to0.70 | % |
Melt mass flow rate | 337°C/6.6kg | ASTMD1238 | 9.5 | g/10min |
K (wear) coefficient | --2 | 内部方法 | 72.0 | |
--3 | 内部方法 | 27.0 | ||
PVLimit4 | 内部方法 | 1.9 | MPa·m/s | |
Density/specific gravity | ASTMD792 | 1.33 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus 5 | ASTMD638 | 3360 | Mpa | |
Bending modulus 7 | 100mmSpan | ASTMD790 | 3410 | Mpa |
Tensile strength 6 | Yield | ASTMD638 | 103 | Mpa |
Elongation rate 6 | Break | ASTMD638 | 40 | % |
FlexuralStrength7 | Yield,100mmSpan | ASTMD790 | 152 | Mpa |
Taber abraser | 1000Cycles,1000g,CS-17Wheel | ASTMD1044 | 2.00 | mg |
friction coefficient | Steel - Dynamic | ASTMD1894 | 0.25 |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
RTIElec | UL746 | 170 | °C | |
Evolution Calendar intelligent importer | UL746 | 170 | °C | |
RTIStr | UL746 | 170 | °C | |
Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTMD648 | 200 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Arc resistance 8 | ASTMD495 | PLC6 | ||
Compared to the anti leakage trace index | CTI | UL746 | PLC4 | |
Hot wire ignition | HWI | UL746 | PLC1 | |
High arc combustion index | HAI | UL746 | PLC0 | |
High voltage arc tracing rate | HVTR | UL746 | PLC2 |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
ReverseNotchIzodImpact | 3.20mm | ASTMD256 | 1300 | J/m |
Impact strength of cantilever beam gap | 23°C | ASTMD256 | 120 | J/m |
23°C | ASTMD4812 | 530 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | M-Scale | ASTMD785 | 110 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.38mm | UL94 | V-0 | |
1.5mm | UL94 | 5VA |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.