PEEK LNP™ THERMOCOMP™ LF-1002 SABIC INNOVATIVE US
86
- Unit Price:
- $75129 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 30MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Hydrolysis resistance Thermal stability
- Application Areas:Electronic and electrical Home appliance components Automotive components
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:24hr | ASTMD955 | 0.30to0.60 | % |
TD:24hr | ASTMD955 | 0.50to0.80 | % | |
Moisture Absorption | 24hr,50%RH | ASTMD570 | 0.070 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.12 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Yield | ISO527-2/5 | 125 | Mpa |
Break | ISO527-2/5 | 122 | Mpa | |
Tensile Strain | Yield | ISO527-2/5 | 3.4 | % |
Break | ISO527-2/5 | 4.0 | % | |
Tensile Elongation | Yield | ASTMD638 | 3.4 | % |
Tensile Modulus | ASTMD638 | 6080 | Mpa | |
Tensile Strength | Break | ASTMD638 | 114 | Mpa |
Yield | ASTMD638 | 120 | Mpa | |
Flexural Modulus | 50.0mmSpan | ASTMD790 | 6010 | Mpa |
Flexural Strength | Yield,50.0mmSpan | ASTMD790 | 203 | Mpa |
Tensile Elongation | Break | ASTMD638 | 4.2 | % |
Flexural Modulus | ISO178 | 5670 | Mpa | |
Tensile Modulus | ISO527-2/1 | 6500 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 326 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 169 | °C | |
Heat Deflection Temperature | 0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 285 | °C |
1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 171 | °C | |
Linear thermal expansion coefficient | MD:-30to30°C | ASTMD696 | 3.5E-05 | cm/cm/°C |
TD:-30to30°C | ASTMD696 | 4.4E-05 | cm/cm/°C |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Multi-Axial Instrumented Impact Energy | ISO6603-2 | 2.50 | J | |
Notched Izod Impact Strength | 23°C | ISO180/1A | 4.6 | kJ/m² |
Unnotched Izod Impact Strength | 23°C | ISO180/1U | 50 | kJ/m² |
Instrumented Dart Impact | 23°C,TotalEnergy | ASTMD3763 | 8.80 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.