PA6T Ultramid®  TKR4357G6 BASF GERMANY

37
  • Unit Price:
    $6378 USD/MT
  • Packaging Specification:
    25KG/PKG
  • Supply Quantity:
    37MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
DensityISO 11831.37g/cm³
Moisture AbsorptionSaturation,23℃ Saturation,23℃ISO 624.5%
Moisture AbsorptionEquilibrium,23℃,50% RH Equilibrium,23℃,50% RHISO 620.8%
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile StrengthBreak,-40℃ Break, -40°FISO 527-2249Mpa
Tensile StrengthBreak,23℃ Break, 73°FISO 527-2165Mpa
Tensile Modulus23℃  23℃ISO 527-29300Mpa
Tensile StrainBreak,-40℃ Break, -40°FISO 527-23.6%
Tensile StrainBreak,23℃ Break, 73°FISO 527-23.5%
ElectricalTest ConditionTest MethodTest ResultUnit
Comparative Tracking IndexIEC 60112600V
Volume ResistivityIEC 60093> 1.0E+15ohms·cm
Dielectric Constant1 MHz  1 MHzIEC 602504.3
Dissipation Factor?1 MHz  1 MHzIEC 602500.03
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Charpy Notched Impact Strength23℃  23°CISO 17919kJ/m²
Notched Izod Impact Strength23℃  23℃ISO 18023kJ/m²
Charpy Unnotched Impact Strength-30℃  -30°CISO 17990kJ/m²
Charpy Unnotched Impact Strength23℃  23°CISO 17995kJ/m²
FlammabilityTest ConditionTest MethodTest ResultUnit
Flame Rating0.75 mm  0.75 mmUL 94HB
Flame Rating1.50 mm  1.5 mmUL 94HB
Flame Rating3.00 mm  3.0 mmUL 94HB
ThermalTest ConditionTest MethodTest ResultUnit
Heat Deflection Temperature1.8 MPa,Unannealed 1.8 MPa,UnannealedISO 75-2/A240°C
Coefficient of Linear Thermal ExpansionTD  TD0.0000551/℃
Tensile Strength0.75 mm  0.75 mmUL 746120°C
Notched Izod Impact Strength0.75 mm  0.75 mmUL 746100°C
Melting temperatureDSC  DSCISO 3146295°C
Coefficient of Linear Thermal ExpansionMD  MD0.0000251/℃
Electrical performance0.75 mm  0.75 mmUL 746140°C
电气性能 1.5 mm  1.5 mmUL 746140°C
电气性能 3.0 mm  3.0 mmUL 746140°C
Tensile Strength1.5 mm  1.5 mmUL 746140°C
Tensile Strength3.0 mm  3.0 mmUL 746140°C
Notched Izod Impact Strength1.5 mm  1.5 mmUL 746110°C
Notched Izod Impact Strength3.0 mm  3.0 mmUL 746115°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.