PA46 Stanyl® TE 200 S6 DSM JAPAN
76
- Unit Price:
- $6564 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 24MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Glass fiber reinforced Thermal stability
- Application Areas:Electronic and electrical Home appliance components
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | Across Flow | ISO 294-4 | 1.7 | % |
流量 | ISO 294-4 | 1.3 | % | |
Moisture Absorption | Equilibrium, 23°C, 50% RH | ISO 62 | 2.6 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile Stress | Break | ISO 527-2 | 90.0 | Mpa |
Break, 120°C | ISO 527-2 | 45.0 | Mpa | |
Break, 160°C | ISO 527-2 | 35.0 | Mpa | |
Break, 180°C | ISO 527-2 | 32.0 | Mpa | |
Break, 200°C | ISO 527-2 | 30.0 | Mpa | |
Tensile Strain | Break | ISO 527-2 | 4.5 | % |
Break, 120°C | ISO 527-2 | 30 | % | |
Break, 160°C | ISO 527-2 | 29 | % | |
Break, 180°C | ISO 527-2 | 28 | % | |
Break, 200°C | ISO 527-2 | 27 | % | |
Tensile Modulus | -- | ISO 527-2 | 4700 | Mpa |
120°C | ISO 527-2 | 1000 | Mpa | |
160°C | ISO 527-2 | 900 | Mpa | |
180°C | ISO 527-2 | 800 | Mpa | |
200°C | ISO 527-2 | 740 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 1.8 MPa, Unannealed | ISO 75-2/A | 235 | °C |
Melting Temperature | ISO 11357-3 | 295 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.