PA46 Stanyl® TW278F10 BK DSM HOLAND
101
- Unit Price:
- $6833 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 11MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability
- Application Areas:Home appliance components Automotive Applications
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | Across Flow | ISO 294-4 | 0.90 | % |
流量 | ISO 294-4 | 0.40 | % | |
Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 1.6 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | -- | ISO 527-2 | 16000 | Mpa |
160°C | ISO 527-2 | 8300 | Mpa | |
200°C | ISO 527-2 | 7600 | Mpa | |
Tensile stress | Break | ISO 527-2 | 235 | Mpa |
Break, 160°C | ISO 527-2 | 120 | Mpa | |
Break, 200°C | ISO 527-2 | 105 | Mpa | |
Tensile strain | Break | ISO 527-2 | 2.2 | % |
Break, 160°C | ISO 527-2 | 3.4 | % | |
Break, 200°C | ISO 527-2 | 3.5 | % | |
Bending modulus | ISO 178 | 12500 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 288 | °C |
1.8 MPa, Unannealed | ISO 75-2/A | 285 | °C | |
Melting temperature 2 | ISO 11357-3 | 290 | °C | |
Linear coefficient of thermal expansion | Flow | ISO 11359-2 | 3.0E-5 | cm/cm/°C |
Across Flow | ISO 11359-2 | 3.0E-5 | cm/cm/°C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 35 | kJ/m² |
23°C | ISO 179/1eU | 55 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.