Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Modeling Shrinkage | Across Flow | ISO 294-4 | 1.0 | % |
Modeling Shrinkage | 流量 | ISO 294-4 | 0.50 | % |
Moisture Absorption | Equilibrium, 23°C, 50% RH | ISO 62 | 2.2 | % |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Stress | Break | ISO 527-2 | 210 | Mpa |
Tensile Stress | Break, 120°C | ISO 527-2 | 100 | Mpa |
Tensile Stress | Break, 160°C | ISO 527-2 | 85.0 | Mpa |
Tensile Stress | Break, 180°C | ISO 527-2 | 75.0 | Mpa |
Tensile Stress | Break, 200°C | ISO 527-2 | 60.0 | Mpa |
Tensile Strain | Break | ISO 527-2 | 3.0 | % |
Tensile Strain | Break, 120°C | ISO 527-2 | 10 | % |
Tensile Strain | Break, 160°C | ISO 527-2 | 11 | % |
Tensile Strain | Break, 180°C | ISO 527-2 | 12 | % |
Tensile Strain | Break, 200°C | ISO 527-2 | 13 | % |
Tensile Modulus | -- | ISO 527-2 | 13000 | Mpa |
Tensile Modulus | 120°C | ISO 527-2 | 5000 | Mpa |
Tensile Modulus | 160°C | ISO 527-2 | 4600 | Mpa |
Tensile Modulus | 180°C | ISO 527-2 | 4200 | Mpa |
Tensile Modulus | 200°C | ISO 527-2 | 3400 | Mpa |
Flexural Modulus | -- | ISO 178 | 13000 | Mpa |
Flexural Modulus | 120°C | ISO 178 | 5000 | Mpa |
Flexural Modulus | 160°C | ISO 178 | 4600 | Mpa |
Flexural Modulus | 180°C | ISO 178 | 4200 | Mpa |
Flexural Modulus | 200°C | ISO 178 | 3400 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Deflection Temperature Under Load? | 0.45 MPa, Unannealed | ISO 75-2/B | 270 | °C |
Deflection Temperature Under Load? | 1.8 MPa, Unannealed | ISO 75-2/A | 256 | °C |
Linear thermal expansion coefficient | Flow | ISO 11359-2 | 2.5E-5 | cm/cm/°C |
Linear thermal expansion coefficient | Across Flow | ISO 11359-2 | 5.0E-5 | cm/cm/°C |
Melting Temperature | | ISO 11357-3 | 282 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Comparative Tracking Index | | IEC 60112 | 300 | V |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | -30°C | ISO 179/1eU | 65 | kJ/m² |
Charpy Unnotched Impact Strength | 23°C | ISO 179/1eU | 90 | kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.