Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melt Volume flow Rate | 235°C/5.0kg | ISO1133 | 14.0 | cm3/10min |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|
Tensile Modulus | | ISO527-2 | 8300 | Mpa |
Flexural Modulus | | ISO178 | 7200 | Mpa |
Tensile Stress | Break | ISO527-2 | 110 | Mpa |
Tensile Strain | Break | ISO527-2 | 4.0 | % |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|
Melting temperature | | ISO11357-3 | 178 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Surface Resistivity | | ISO3915 | <1.0E+5 | ohms |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|
Charpy Unnotched Impact Strength | -30°C | ISO179 | NoBreak | |
Charpy Unnotched Impact Strength | 23°C | ISO179 | NoBreak | |
Supplementary information | Test Condition | Test Method | Test Result | Unit |
---|
ISO Shortname | | ISO1874 | PA12,MHLR,18-080,CF15 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.