Need Help? Contact Us service@plas.com
Get App

PBT T08 200 DSM HOLAND

43
  • Unit Price:
    $4283 USD/MT
  • Packaging Specification:
    25KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Moisture AbsorptionSaturation,23°CISO620.45%
Moisture AbsorptionEquilibrium,23°C,50%RHISO620.18%
Melt Volume flow Rate250°C/2.16kgISO113310.0cm3/10min
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Nominal Tensile Strain at BreakISO527-2>50%
Tensile StressYieldISO527-255.0Mpa
Tensile StrainYieldISO527-23.5%
Tensile ModulusISO527-22550Mpa
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Deflection Temperature Under Load?0.45MPa,UnannealedISO75-2/B170°C
Deflection Temperature Under Load?1.8MPa,UnannealedISO75-2/A55.0°C
Linear thermal expansion coefficientMDISO11359-29E-05cm/cm/°C
Linear thermal expansion coefficientTDISO11359-29E-05cm/cm/°C
Melting TemperatureISO11357-3225°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
Relative Permittivity100HzIEC602503.50
Relative Permittivity1MHzIEC602503.20
Comparative Tracking IndexIEC60112600V
Dielectric StrengthIEC60243-127KV/mm
Dissipation Factor?100HzIEC602502E-03
Dissipation Factor?1MHzIEC602500.020
Volume ResistivityIEC60093>1.0E+15ohms·cm
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Charpy Unnotched Impact Strength-30°CISO179/1eUNoBreak
Charpy Unnotched Impact Strength23°CISO179/1eUNoBreak
FlammabilityTest ConditionTest MethodTest ResultUnit
UL flame retardant rating0.75mmIEC60695-11-10,-20HB
UL flame retardant rating1.5mmIEC60695-11-10,-20HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.