Need Help? Contact Us service@plas.com
Get App

PBT LNP™ LUBRICOMP™  WL004 WHNAT SABIC INNOVATIVE US

39
  • Unit Price:
    $4477 USD/MT
  • Packaging Specification:
    25KG/PKG
  • Supply Quantity:
    70.5MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

serv********

For more detailed information including pricing, customization, and shipping, please contact supplier.

Technical Data Sheet

Physical PropertiesTest ConditionTest MethodTest ResultUnit
Modeling ShrinkageMD:24hrASTMD9552.1to2.4%
Modeling ShrinkageTD:24hrASTMD9552.1to2.4%
Modeling ShrinkageTD:24hrISO294-42.1to2.3%
Modeling ShrinkageMD:24hrISO294-42.4to2.5%
Moisture Absorption24hr,50%RHASTMD5700.051%
Moisture AbsorptionEquilibrium,23°C,50%RHISO620.080%
Mechanical PropertiesTest ConditionTest MethodTest ResultUnit
Tensile StressBreakISO527-245.0Mpa
Tensile StrainBreakISO527-28.4%
Tensile ModulusISO527-2/12450Mpa
Tensile ElongationBreakASTMD6389.8%
Flexural ModulusASTMD7902410Mpa
Flexural ModulusISO1782390Mpa
Flexural StrengthASTMD79078.7Mpa
Flexural StressISO17877.1Mpa
Coefficient of FrictionDynamicASTMD3702Modified0.33
Coefficient of FrictionStaticASTMD3702Modified0.24
Tensile ModulusASTMD6382410Mpa
Tensile StrengthBreakASTMD63849.0Mpa
Specific Wear RateASTMD3702Modified58.010^-10in^5-min/ft-lb-hr
Thermal PropertiesTest ConditionTest MethodTest ResultUnit
Heat Deflection Temperature1.8MPa,Unannealed,64.0mmSpanISO75-2/Af61.0°C
Deflection Temperature Under Load?1.8MPa,Unannealed,3.20mmASTMD64855.0°C
Linear thermal expansion coefficientMD:-40to40°CISO11359-29E-05cm/cm/°C
Linear thermal expansion coefficientTD:-40to40°CASTME8319.6E-05cm/cm/°C
Linear thermal expansion coefficientTD:-40to40°CISO11359-29.6E-05cm/cm/°C
Linear thermal expansion coefficientMD:-40to40°CASTME8319E-05cm/cm/°C
Impact PropertiesTest ConditionTest MethodTest ResultUnit
Multi-Axial Instrumented Impact EnergyISO6603-20.500J
Notched Izod Impact Strength23°CISO180/1A3.6kJ/m²
UnnotchedIzodImpactStrength323°CISO180/1U30kJ/m²
Instrumented Dart Impact23°C,EnergyatPeakLoadASTMD37630.960J
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.