PBT VALOX™ 420SE0-8051 SABIC INNOVATIVE US
77
- Unit Price:
- $3670 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 15.1MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Glass fiber reinforced high strength
- Application Areas:Office supplies Electronic accessories
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | MD:--2 | 内部方法 | 0.10to0.50 | % |
MD:3.20mm | 内部方法 | 0.50to0.70 | % | |
TD:--2 | 内部方法 | 0.40to0.80 | % | |
TD:3.20mm | 内部方法 | 0.50to1.0 | % | |
Moisture Absorption | Saturation,23°C | ISO62 | 0.090 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.070 | % | |
Melt Mass-Flow Rate | 250°C/5.0kg | ASTMD1238 | 42 | g/10min |
Melt Volume flow Rate | 250°C/5.0kg | ISO1133 | 29.0 | cm3/10min |
Specific Volume | ASTMD792 | 0.610 | cm³/g | |
Outdoor Suitability | UL746C | f2 | ||
Density / Specific Gravity | ASTMD792 | 1.63 | g/cm³ | |
ISO1183 | 1.63 | g/cm³ |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Modulus | 50.0mmSpan | ASTMD790 | 9800 | Mpa |
Flexural Strength | Break,50.0mmSpan | ASTMD790 | 186 | Mpa |
Tensile Strength | Yield | ASTMD638 | 120 | Mpa |
Tensile Modulus | ASTMD638 | 12000 | Mpa | |
Tensile Strength | Break | ASTMD638 | 120 | Mpa |
Flexural Modulus | ISO178 | 9500 | Mpa | |
Flexural Stress | ISO178 | 180 | Mpa | |
Tensile Elongation | Break | ASTMD638 | 2.0 | % |
Yield | ASTMD638 | 2.0 | % | |
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17Wheel | 内部方法 | 22.0 | mg |
Tensile Stress | Break | ISO527-2/5 | 120 | Mpa |
Yield | ISO527-2/5 | 120 | Mpa | |
Tensile Strain | Yield | ISO527-2/5 | 1.9 | % |
Break | ISO527-2/5 | 1.9 | % | |
Tensile Modulus | ISO527-2/1 | 10000 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Deflection Temperature Under Load? | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 212 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 200 | °C | |
1.8MPa,Unannealed,100mmSpan9 | ISO75-2/Ae | 195 | °C | |
1.8MPa,Unannealed,64.0mmSpan10 | ISO75-2/Af | 200 | °C | |
Vicat Softening Temperature | ASTMD152511 | 200 | °C | |
-- | ISO306/A50 | 220 | °C | |
-- | ISO306/B50 | 200 | °C | |
-- | ISO306/B120 | 200 | °C | |
Linear thermal expansion coefficient | MD:-40to40°C | ASTME831 | 2.5E-05 | cm/cm/°C |
MD:-40to40°C | ISO11359-2 | 2.5E-05 | cm/cm/°C | |
MD:23to80°C | ISO11359-2 | 2.5E-05 | cm/cm/°C | |
TD:-40to40°C | ASTME831 | 8.9E-05 | cm/cm/°C | |
TD:-40to40°C | ISO11359-2 | 8.9E-05 | cm/cm/°C | |
TD:23to80°C | ISO11359-2 | 1.2E-04 | cm/cm/°C | |
RTIElec | UL746 | 130 | °C | |
Evolution Calendar intelligent importer | UL746 | 130 | °C | |
RTIStr | UL746 | 140 | °C | |
Thermal Conductivity | ISO8302 | 0.25 | W/m/K | |
Ball PressureTest | 125°C | IEC60695-10-2 | Pass | |
Heat Deflection Temperature | 0.45MPa,Unannealed,100mmSpan | ISO75-2/Be | 220 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Arc Resistance | ASTMD495 | PLC6 | ||
Relative Permittivity | 50Hz | IEC60250 | 3.30 | |
60Hz | IEC60250 | 3.30 | ||
100Hz | IEC60250 | 3.80 | ||
1MHz | IEC60250 | 3.30 | ||
Comparative Tracking Index | -- | IEC60112 | 175 | V |
SolutionB | IEC60112 | 125 | V | |
Hot-wire Ignition | HWI | UL746 | PLC2 | |
Dielectric Strength | 1.60mm,in Oil | ASTMD149 | 24 | KV/mm |
3.20mm,inAir | ASTMD149 | 19 | KV/mm | |
0.800mm,in Oil | IEC60243-1 | 23 | KV/mm | |
1.60mm,in Oil | IEC60243-1 | 22 | KV/mm | |
3.20mm,in Oil | IEC60243-1 | 16 | KV/mm | |
Comparative Tracking Index | CTI | UL746 | PLC3 | |
High Amp Arc Ignition | HAI | UL746 | PLC0 | |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC4 | |
Dissipation Factor? | 100Hz | ASTMD150 | 2E-03 | |
1MHz | ASTMD150 | 0.020 | ||
50Hz | IEC60250 | 1E-03 | ||
60Hz | IEC60250 | 1E-03 | ||
100Hz | IEC60250 | 2E-03 | ||
1MHz | IEC60250 | 0.010 | ||
Surface Resistivity | IEC60093 | >1.0E+15 | ohms | |
Dielectric Constant | 100Hz | ASTMD150 | 3.80 | |
1MHz | ASTMD150 | 3.70 | ||
Volume Resistivity | ASTMD257 | >1.0E+15 | ohms·cm | |
IEC60093 | >1.0E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Unnotched Izod Impact Strength | -30°C | ISO180/1U | 45 | kJ/m² |
23°C | ISO180/1U | 45 | kJ/m² | |
Instrumented Dart Impact | 23°C,TotalEnergy | ASTMD3763 | 5.00 | J |
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 6.0 | kJ/m² |
23°C | ISO179/1eA | 7.0 | kJ/m² | |
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 50 | kJ/m² |
23°C | ISO179/1eU | 50 | kJ/m² | |
Notched Izod Impact Strength | -30°C | ISO180/1A | 6.0 | kJ/m² |
23°C | ISO180/1A | 7.0 | kJ/m² | |
Notched Izod Impact Strength | 23°C | ASTMD4812 | 620 | J/m |
-30°C | ASTMD256 | 57 | J/m | |
23°C | ASTMD256 | 60 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell Hardness | R-Scale | ASTMD785 | 119 | |
R-Scale | ISO2039-2 | 119 | ||
Ball Indentation Hardness | H358/30 | ISO2039-1 | 118 | Mpa |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Oxygen Index | ISO4589-2 | 32 | % | |
UL flame retardant rating | 0.40mm | UL94 | V-2 | |
0.71mm | UL94 | V-0 | ||
2.0mm | UL94 | 5VA | ||
Glow Wire Flammability Index | 1.0mm | IEC60695-2-12 | 960 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.