PBT Cristin® S650FR NC010 DUPONT USA
90
- Unit Price:
- $3863 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 61.5MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515
serv********
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant
- Application Areas:Electronic and electrical
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
Physical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Modeling Shrinkage | TD2 | ISO294-4 | 2.2 | % |
TD | ISO294-4 | 1.6 | % | |
MD | ISO294-4 | 1.8 | % | |
MD2 | ISO294-4 | 2.2 | % | |
Moisture Absorption | Saturation,23°C,2.00mm | ISO62 | 0.39 | % |
Equilibrium,23°C,2.00mm,50%RH | ISO62 | 0.15 | % | |
Ejection Temperature | 170 | °C |
Mechanical Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flexural Stress | ISO178 | 100 | Mpa | |
Nominal Tensile Strain at Break | ISO527-2 | 7.2 | % | |
Tensile Stress | Yield | ISO527-2 | 65.0 | Mpa |
Tensile Strain | Yield | ISO527-2 | 4.6 | % |
Tensile Creep Modulus | 1000hr | ISO899-1 | 1800 | Mpa |
Tensile Modulus | ISO527-2 | 3000 | Mpa | |
Tensile Creep Modulus | 1hr | ISO899-1 | 2500 | Mpa |
Thermal Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat Softening Temperature | ISO306/B50 | 175 | °C | |
Deflection Temperature Under Load? | 0.45MPa,Unannealed | ISO75-2/B | 160 | °C |
1.8MPa,Unannealed | ISO75-2/A | 65.0 | °C | |
Linear thermal expansion coefficient | MD | ISO11359-2 | 1.2E-04 | cm/cm/°C |
TD | ISO11359-2 | 1.2E-04 | cm/cm/°C | |
Melting Temperature | ISO11357-3 | 221 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric Strength | IEC60243-1 | 25 | KV/mm | |
Relative Permittivity | 100Hz | IEC60250 | 3.40 | |
1MHz | IEC60250 | 3.50 | ||
Comparative Tracking Index | IEC60112 | 225 | V | |
Dissipation Factor? | 100Hz | IEC60250 | 7.1E-04 | |
1MHz | IEC60250 | 0.018 | ||
Surface Resistivity | IEC60093 | 1E+15 | ohms | |
Volume Resistivity | IEC60093 | >1.0E+15 | ohms·cm |
Impact Properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Unnotched Impact Strength | -30°C | ISO179/1eU | 65 | kJ/m² |
23°C | ISO179/1eU | 70 | kJ/m² | |
Notched Izod impact strength | -30°C | ISO180/1U | 42 | kJ/m² |
23°C | ISO180/1U | 45 | kJ/m² |
Flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.75mm | UL94 | V-0 | |
1.5mm | UL94 | V-0 | ||
0.75mm | IEC60695-11-10,-20 | V-0 | ||
1.5mm | IEC60695-11-10,-20 | V-0 | ||
Oxygen Index | ISO4589-2 | 30 | % | |
FMVSS Flammability | FMVSS302 | DNI |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.